Q345b +304 L plak asye clad

Q345b +304 L plak asye clad

Lajè: max2500mm
Epesè: epesè total: 5-50mm
(CLADDING materyèl epesè: 1-10mm)
Longè: max15000mm
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik
 

Q345b +304 L clad asye plak konpozisyon chimik ak pwopriyete mekanik

 

 

Egalize C % Si % Mn P % S %  
Q345B Mwens pase oswa egal a 0.20 Mwens pase oswa egal a 0.55 1.00-1.60 Mwens pase oswa egal a 0.040 Mwens pase oswa egal a 0.040  
             
Egalize Epesè Sede fòs (MPa) Fòs rupture Elongasyon Enpak enèji
(mm) (MPA) (%) Min
Q345B Mwens pase oswa egal a 16 345 470-630 21 20 34J
>16-35 325 470-630 21 20 34J
>35 295 470-630 21 20 34J
Enèji nan enpak min se enèji Longitudinal

 

Egalize

 

C

 

Mn

 

P

 

 

S

 

 

Si

 

Cr

NI Mwa NI

 

Koper

 

304L(S30403) 0.030 2.0 0.045 0.030 0.75 17.5-19.5 8.0-12.0 - 0.10 -

 

Egalize

Sede fòs

(N/mm2), min

Fòs rupture (N/mm2), min

Elongationin 2 pous (50mm), %, min
Dite, Max
Brinell Rockwell B
Fwad Bend

Austenitic (CHROMIUM - NICKEL) (CHROMIUM - Manganese - Nickel)

304L(S30403)
25 170
70 485
40
201 92
pa obligatwa

 

 

Q345b +304 l aplikasyon plak asye clad

 

 

Q345B +304 L plak asye yo te itilize nan konstriksyon nan pon, konstriksyon gran wout ak lòt konstriksyon jeni.

 

 

Q345b +304 l plak asye clad lòt non

 

 

Q345b +304 L plak asye clad, Q345B plak asye, 304L plak asye

 

 

Lòt kondisyon

 

 

UT (egzamen ultrasons), AR (tankou cho woule sèlman), TMCP (tèmik pwosesis kontwòl mekanik), N (normalized), Q+T (pasè ak apeze), z tès direksyon (Z15, Z25, Z35), Charpy V - tès enpak, tankou SG.

Mande pou karakteristik CSP

Pou veso presyon idwojèn depo ki egzije rezistans idwojèn embrittlement, nou bay s355jr +304 l rekouvèr asye ak lòt klas reyinyon GB/t 34510.

Imèl:alloy@gneesteelgroup.com

WhatsApp (WeChat): +86 15824687445

 

Baj popilè: q345b +304 l plak asye clad, Lachin Q345b {{3}