P265GH +410 CLAD asye plak konpozisyon chimik ak pwopriyete mekanik
|
Egalize |
Konpozisyon chimik (%) |
||||
|
C max |
Mn |
Si max |
P Max |
S max |
|
|
EN10028-2 P265GH |
0.2 |
0.8-1.4 |
0.40 |
0.025 |
0.015 |
|
Egalize |
Pwopriyete mekanik |
|
|||
|
Fòs rupture (MPa) |
Sede fòs (MPa) min |
Elongasyon nan 2 pous (50mm) min |
Enpak tanperati tès la (degre) |
|
|
|
EN10028-2 P265GH |
390-530 |
265 |
22 |
+20,0,-20 |
|
| Egalize |
C
|
Mn |
P
|
S
|
Si |
Cr |
NI | Mwa | NI |
Koper
|
| 410(S41000) | 0.08-0.15 | 1.00 | 0.040 | 0.030 | 1.00 | 11.5-13.5 | 0.75 | - | - | - |
| Egalize |
Sede fòs (N/mm2), min |
Fòs rupture (N/mm2), min |
Elongationin 2 pous (50mm), %, min |
|
Fwad Bend | ||||||
|
Austenitic (CHROMIUM - Nikèl) (CHROMIUM - Manganese - Nickel) |
|||||||||||
| 410(S41000) |
|
|
20 |
|
180 | ||||||

P265GH +410 plak asye rekouvèr yo te itilize nan konstriksyon nan pon, konstriksyon gran wout ak lòt konstriksyon jeni.
P265GH +410 Plak Steel CLAD lòt non
P265GH +410 Plak Steel CLAD, plak asye P265GH, 410 plak asye


Steel GNEE se manifakti dirijan nan mond lan nan woulo liv - plak ki lye ak rekouvèr. Nou ofri plak rekouvèr, tèt rekouvèr ak kòn rekouvèr.Kòm yon manifakti ak plizyè dekad nan eksperyans nan lyezon woulo liv, nou se patnè serye ou nan linepipe a, veso presyon ak endistri aparèy.
Baj popilè: P265GH +410 Plak Steel CLAD, Lachin P265GH {{3}