P265GH+904L Plak Asye Rekouvèt

P265GH+904L Plak Asye Rekouvèt

Lajè: Max 2500mm
Epesè: epesè total: 5-50mm
(Epesè materyèl CLADDING: 1-10mm)
Longè: Max 15000mm
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

P265GH+904L plak asye rekouvèr konpozisyon chimik ak pwopriyete mekanik

 

P265GH konpozisyon chimik

Klas

Eleman Max (%)

C

Si

Mn

P

S

Al(min)

N

P265GH

0.20

0.40

0.80-1.40

0.025

0.015

0.020

0.012

Kr

Cu

Mo

Nb

Ni

Ti

V

0.30

0.30

0.08

0.020

0.30

0.03

0.02

 

Klas

 

P265GHPwopriyete mekanik

Epesè

Sede

Tensilmie

Elongasyon

Enèji enpak (KV J) min

P265GH

mm

Min Mpa

Mpa

% min

-20 degre

0 degre

+20 degre

Mwens pase oswa egal a 16

265

410-530

22

27

34

40

16>a mwens pase oswa egal a 40

255

410-530

22

27

34

40

40>a mwens pase oswa egal a 60

245

410-530

22

27

34

40

60>a mwens pase oswa egal a 100

215

410-530

22

27

34

40

100>a mwens pase oswa egal a 150

200

400-530

22

27

34

40

150>a mwens pase oswa egal a 250

185

390-530

22

27

34

40

 

Klas

 

C

 

Mn

 

P

 

 

S

 

 

Si

 

Kr

Ni Mo Ni

 

Cooper

 

904L(N08804) 0.020 2.00 0.045 0.035 1.00 19.0-23.0 23.0-28.0 4.00-5.00 0.10 1.00-2.00
Klas

Sede fòs

(N/mm2), min

Fòs rupture (N/mm2), min

Elongasyon nan 2 pous (50mm), %, min
Dite, max
Brinell Rockwell B
Fwad koube

Austenitic (Kwòm-Nikèl) (Kwòm-Manganèz-Nikèl)

904L(N08804)
31 220
71 490
35
- 90
pa obligatwa

 

P265GH+904L Plak asye rekouvèr Aplikasyon

 

P265GH+904L plak asye ki kouvri yo itilize nan konstriksyon pon, konstriksyon otowout ak lòt konstriksyon jeni.

 

P265GH+904L Plak asye rekouvèr Lòt Non

 

P265GH+904L plak asye plak, plak asye P265GH, plak asye 904L

 

Kondisyon adisyonèl

 

UT (Egzamen Ultrasonic), AR (Kòm woule cho sèlman), TMCP (Tèmik Pwosesis kontwòl mekanik), N (Normalize), Q + T (Tenn ak Tanperaman), Tès Direksyon Z (Z15, Z25, Z35), Tès Enpak Charpy V - Notch, Tès Twazyèm Pati (tankou Tès SGS), kouvwi ak pating.

Kontakte pou CSP

 

Pou veso presyon idwojèn depo ki mande rezistans idwojèn frajilman, nou bay S355JR+304L Clad asye ak lòt klas ki satisfè GB/T 34510. Si ou bezwen verifye rezilta tès Hydrogen Induced Cracking (HIC), konsepsyon presyon adaptabilite, oswa Customize solisyon ki lejè, kontakte pou kominikasyon ak sitasyon eksklizif.

Imèl:alloy@gneesteelgroup.com

Whatsapp (WeChat): +86 15824687445

 

product-376-293product-315-225

product-299-270product-365-374

product-385-328product-324-337

 

Baj popilè: p265gh+904l rekouvèr plak asye, Lachin p265gh+904l rekouvèr plak asye manifaktirè, founisè, faktori