DIN 17155 10 CRMO910 pou plak veso presyon

DIN 17155 10 CRMO910 pou plak veso presyon

DIN 17155 10 CRMO910 veso presyon ak plak asye chodyè yo te itilize nan veso presyon, chofaj, tank depo ak echanjeur chalè nan lwil oliv, pwojè gaz.
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

Konpozisyon chimik ak pwopriyete mekanik

Egalize C% Si% Mn% P%, max S%, max Al% Cr% Cu%, max Mo% Nb%, max Ni%, max Ti%, max V%, max
10crmo910 0.06-0.15 Mwens pase oswa egal a O.50 0.4-0.7 0.035 0.03   2-2.5 0.3 0.9-1.1        
Klas asye Epesè, nan mm Sede fòs, min Fòs rupture Elongasyon, %, min
10crmo910 T mwens pase oswa egal a 16 310 480-630 18
16<> 300
40<> 290
60<> 270 460-630 17
100<> 250 460-630

 

1. Ki sa ki pwopriyete yo kle mekanik nan 10CRMO910 plak?

Repons:
10crmo910 se yonsegondè-klas CHROMIUM-MOLYBDENUM asyeAvèk:

Fòs rupture: 480-630 MPa

Sede fòs: Pi gran pase oswa egal a 310 MPa

Elongasyon: Pi gran pase oswa egal a 18% (pou t mwens pase oswa egal a 16mm)

Enpak andirans: Pi gran pase oswa egal a 40J nan 20 degre

Epesè Range: 5-250mm

Tanperati sèvis maksimòm: 600 degre


2. Kijan konpozisyon 10crmo910 la diferan de 13crmo44?

Repons:
Kle diferans konpozisyon:

Eleman 10crmo910 13crmo44 Efè
Cr 2.00-2.50% 0.70-1.15% Amelyore rezistans oksidasyon
Mwa 0.90-1.10% 0.40-0.60% Fòs ranpe siperyè
C 0.08-0.14% 0.10-0.18% Pi bon soudabilite

3. Ki tretman chalè obligatwa?

Repons:
Pwosesis obligatwa:

Nòmalize: 930-980 degre

Tanperaman: 680-780 degre (minimòm 2hrs/25mm)

Volontè: Fo PWHT pou aplikasyon nikleyè


4. Ki kondisyon soude kritik yo?

Repons:
Pwotokòl esansyèl soude:

Chèz: 250-300 degre (konsève jouk PWHT)

Consommables: DIN 8556 E CRMO 9 1 0

Entèrpass temp: 300-350 degre

PWHT: Obligatwa (700-750 degre × 3hrs + 1 HR/25mm)

Kontwòl dite: Mwens pase oswa egal a 241 Hb


5. Ki kote 10crmo910 esansyèl?

Repons:
Aplikasyon kritik:

Réacteurs hydrocracking(200+ ba)

Bato likid chabon

Chodyè ultra-supercritical

Dèlko vapè nikleyè

High-presyon sistèm idwojèn


Konparezon pèfòmans

Egalize CR kontni Max temp Estanda ekivalan
10crmo910 2.0-2.5% 600 degre ASTM A387 Gr.22
13crmo44 0.7-1.15% 550 degre En 10028-2 13 CRMO4-5
16mo3 Okenn 525 degre En 10028-2 16 Mo3

Baj popilè: DIN 17155 10 CRMO910 pou plak veso presyon, Lachin DIN 17155 10 CRMO910 pou manifaktirè plak veso presyon, founisè, faktori