Cr5mo1v skd12 wonn baton metal

Cr5mo1v skd12 wonn baton metal

Pwodwi: CR5MO1V SKD12 wonn baton metal
Shap: wonn
Longè: Kondisyon Kliyan yo
Tolerans: ± 1%
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

Cr5mo1v skd12 wonn baton metal


CR5MO1V se yon kabòn segondè, mwayen CHROMIUM, yon ti kras defòme lè - fè tèt di frèt travay asye mwazi ak asye zouti alyaj. The steel due to air quenching caused by the deformation of only manganese-containing oil quenching tool steel about 1/4, wear resistance between manganese-type and high-carbon, high-chromium tool steel, its toughness is better than any kind of good, especially suitable for the requirements of good wear resistance at the same time with special Bon severite nan zouti a, lajman ki itilize nan mouri a mouri ak fòme mouri, woulo, pwenson, kalandriye mwazi ak woule mouri, tou yo itilize nan kèk kalite lam sizo.

 

Corresponding grades: China GB standard grade Cr5Mo1V, Japan standard grade SKD12, Sweden ASSAB (ASSAB) standard grade XW-10, China Taiwan CNS standard grade SKD12, South Korea KS standard grade STD12, the US ASTM / UNS standard grade A2/T30102, the International Organisation for Standardisation (ISO) standard grade 100CrMoV early, Germany DIN standard grade X100CrMoV5-1, Alman DIN Creole Materyèl Nimewo 1.2363, Lafrans NF Creole Klas X100CRMOV5, Syèd SS Creole Klas 2260, Britanik BS estanda klas BA2.

 

 
Cr5mo1v solid asye wonn ba konpozisyon chimik

 

C(%) Si (%) MN (%) P(%) S(%) Cr (%) Ni (%) Mo (%) V(%) Cu (%)
0.95-1.05 Mwens pase oswa egal a 0.50 Mwens pase oswa egal a 1.00 Mwens pase oswa egal a 0.030 Mwens pase oswa egal a 0.030 4.75-5.50 Mwens pase oswa egal a 0.20 0.90-1.40 0.15-0.50 Mwens pase oswa egal a 0.30

 

 
Cr5mo1v solid wonn bar asye pwopriyete mekanik

 

Prèv Fòs
RP0.2 (MPa)
Fòs rupture
RM (MPA)
Enpak enèji
KV (J)
Elongasyon nan ka zo kase
A(%)
Rediksyon nan koup transvèsal sou ka zo kase
Z(%)
Kòm - chalè - kondisyon trete Brinell dite (HBW)
828 (pi gran pase oswa egal a) 147 (pi gran pase oswa egal a) 21 44 22 Solisyon ak aje, rkwir, ausaging, q+t, elatriye 221

 

 
cr5mo1v wonn ba pwopriyete fizik

 

Tanperati
(degre)
Modil Elastisite
(GPA)
Vle di koyefisyan nan ekspansyon tèmik 10-6/(degre) ant 20 (degre) ak Kapasite tèmik espesifik
(J/kg · degre)
Espesifik rezistivite elektrik
(Ω mm²/m)
Densite
(kg/dm³)
Koyefisyan Poisson a, ν Konduktiviti tèmik
(W/m · degre)
22   0.32    
251 588 214     42.3
173 21     432 431 41.2

 

 
Steel wonn ba pwodwi imaj

 

China steel round bar Distributors

 

 
Gnee Group Ekip foto

 

China round stock steel Suppliers

 

 
Gnee Gwoup Kliyan Vizit

 

China round bar stock Manufacturers

 

 
Gnee Group patisipe nan egzibisyon pwodwi asye

 

China round metal bar Distributors

Nou ka garanti tan livrezon. Si ou gen bezwen personnalisation pou CR5MO1V SKD12 wonn baton metal oswa lòt jij asye klas, tanpri kontakte m '.

 

Baj popilè: cr5mo1v SKD12 wonn baton metal, Lachin CR5MO1V SKD12 Round Metal Rod Konpayi fabrikasyon, Swèd, faktori