9Mn2V SKS31 Steel Rod Bar
9Mn2V wonn asye se yon kalite asye zouti alyaj ki ba ak pi bon pwopriyete mekanik konplè pase asye zouti kabòn, li gen gwo dite ak rezistans mete. Deformation pandan trempe se ti ak hardenability a trè bon. Kòm asye a gen yon sèten kantite vanadyòm, rafine grenn nan, diminye sansiblite a surchof nan asye a. An menm tan an carbure yo pi rafine ak plis respire distribye.
Nimewo asye apwoksimatif etranje: 90MnV2 (ISO), O2 (ASTM), T31502 (UNS), 90MnV8 (EN), 105WCr1 (ISO), SKS31 (JIS), STS31 (KS), 107WCr5 (EN), 105WCr6 (DIN).
9Mn2V SKS31 wonn metal stock chimik compisiton
| ASTM A681 | C | Si | Mn | P | S | Kr | Mo | V |
| O2/T31502 | 0.85-0.95 | Mwens pase oswa egal a 0.50 | 1.40-1.80 | 0.030 Max | 0.030 Max | Mwens pase oswa egal a 0.50 | Mwens pase oswa egal a 0.30 | Mwens pase oswa egal a 0.30 |
| DIN 17350 | C | Si | Mn | P | S | Kr | Mo | V |
| 1.2842/90MnCrV8 | 0.85-0.95 | 0.10-0.40 | 1.90-2.10 | 0.035 Max | 0.035 Max | 0.20-0.50 | - | 0.05-0.15 |
| GB/T 1299 | C | Si | Mn | P | S | Kr | Mo | V |
| 9Mn2V | 0.85-0.95 | Mwens pase oswa egal a 0.40 | 1.70-2.00 | 0.030 Max | 0.030 Max | Mwens pase oswa egal a 0.25 | ~ | Mwens pase oswa egal a 0.20 |
| JIS SKS31 | C | Si | Mn | P | S | Kr | Mo | V |
9Mn2V wonn metal baton pwopriyete mekanik
| Sede Fòs Rp0.2(MPa) |
Fòs rupture Rm(MPa) |
Enèji enpak AKV(J) |
Elongasyon nan Frakti A(%) |
Rediksyon nan koup transvèsal sou Frakti Z(%) |
Valè rezistans enpak kv (J/cm2) | Dite (Brinell) |
|---|---|---|---|---|---|---|
| Pi gran pase oswa egal a 928 | Pi gran pase oswa egal a 962 | Pi gran pase oswa egal a 43 |
Pi gran pase oswa egal a 12 |
Pi gran pase oswa egal a 55 |
Pi gran pase oswa egal a 44 |
Mwens pase oswa egal a 343 |
9Mn2V solid asye wonn pwopriyete fizik
| Tanperati (degre) |
Modil elastisite (GPa) |
Mwayèn koyefisyan ekspansyon tèmik 10-6/(degre) ant 20(degre) ak | Konduktivite tèmik (W/m· degre) |
Kapasite tèmik espesifik (J/kg· degre) |
Espesifik rezistans elektrik (Ω mm²/m) |
Dansite (kg/dm³) |
Koyefisyan Poisson a, ν |
|---|---|---|---|---|---|---|---|
| 12 | - | - | 0.41 | - | |||
| 281 | 168 | - | 32.3 | 333 | - | ||
| 693 | - | 21 | 21.2 | 422 | 211 |
solid wonn ba asye Pwodwi imaj

Foto ekip gwoup GNEE

Vizit kliyan gwoup GNEE

Gwoup GNEE patisipe nan egzibisyon pwodwi asye

Nou gen plis pase 15 ane eksperyans nan pwodiksyon ak ekspòtasyon. Si ou gen nenpòt bezwen Customized pou 9Mn2V SKS31 Steel Rod Bar oswa lòt plak asye cho -woule, tanpri kontakte m.
Baj popilè: 9mn2v sks31 asye baton bar, Lachin 9mn2v sks31 asye baton bar manifaktirè, Swèd, faktori