P355QH chodyè bon jan kalite plak
P355QH asye chodyè plak se yon kalite wo -tanperati presyon veso asye plak espesifye nan estanda Ewopeyen an EN 10028 -6.P355QH plak veso presyon gen gwo fòs ak rezistans tanperati ki wo, ki se apwopriye pou fabrikasyon wo-tanperati veso presyon ak chodyèr ak lòt ekipman.
Plak asye presyon veso P355QH nou ofri a ka Customized nan gwosè, koupe, soude, pwensonaj ak lòt sèvis pwosesis dapre kondisyon fen -itilize ou pou pwodwi materyèl plak veso presyon P355QH.
presyon veso plak materyèl ChimikKonpozisyon
| C | Si | Mn | P | S | Ni | Kr | Mo | Cu | Nb | V | Ti | N | Zr | B |
| Mwens pase oswa egal a 0.16 | Mwens pase oswa egal a 0.4 | Mwens pase oswa egal a 1.5 | Mwens pase oswa egal a 0.025 | Mwens pase oswa egal a 0.015 | Mwens pase oswa egal a 0.5 | Mwens pase oswa egal a 0.3 | Mwens pase oswa egal a 0.25 | Mwens pase oswa egal a 0.3 | Mwens pase oswa egal a 0.05 | Mwens pase oswa egal a 0.06 | Mwens pase oswa egal a 0.03 | Mwens pase oswa egal a 0.015 | Mwens pase oswa egal a 0.05 | Mwens pase oswa egal a 0.005 |
veso asye plak pwopriyete mekanik
| Klas | Eta livrezon | Epesè mm | Pwopriyete mekanik | |
| P355QH | trempe ak tanperaman | <5 | ReH (MPa) | Pi gran pase oswa egal a 355 |
| Rm (MPa) | 490-630 | |||
| A(%) | Pi gran pase oswa egal a 22 | |||
| P355QH | 5~50 | ReH (MPa) | Pi gran pase oswa egal a 355 | |
| Rm (MPa) | 490-630 | |||
| A(%) | Pi gran pase oswa egal a 22 | |||
| Enpak tanperati degre | -20 | |||
| Akv(J) | Pi gran pase oswa egal a 27 | |||
| P355QH | >50~100 | ReH (MPa) | Pi gran pase oswa egal a 335 | |
| Rm (MPa) | 490-630 | |||
| A(%) | Pi gran pase oswa egal a 22 | |||
| Enpak tanperati degre | -20 | |||
| Akv(J) | Pi gran pase oswa egal a 27 | |||
| P355QH | >100~150 | ReH (MPa) | Pi gran pase oswa egal a 315 | |
| Rm (MPa) | 450-590 | |||
| A(%) | Pi gran pase oswa egal a 22 | |||
| Enpak tanperati degre | -20 | |||
| Akv(J) | Pi gran pase oswa egal a 27 | |||
chodyè asye Pwodwi imaj

Foto ekip gwoup GNEE

Vizit kliyan gwoup GNEE

GNEE Group asye egzibisyon

Nou gen ekselan apre-lavant sèvis. Si ou gen nenpòt kesyon sou plak bon jan kalite chofaj P355QH, ou ka kontakte nou epi nou pral reponn ou nan de zè de tan.
Baj popilè: p355qh chodyè bon jan kalite plak, Lachin p355qh chodyè bon jan kalite plak manifaktirè, Swèd, faktori