P295GH cho woule presyon veso Steel Plak

P295GH cho woule presyon veso Steel Plak

Kalite: Presyon Veso (PVQ) Steel Plak
Estanda: AISI, ASTM, DIN, JIS, GB
Teknik: Woule cho
Fòm: Plak
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

P295GH cho woule presyon veso Steel Plak


 

GNEE se yon founisè plak veso P295GH ki gen 16 ane eksperyans nan fabrikasyon, plak chodyè P295GH nou ofri yo fabrike an akò strik ak estanda a, te pase sètifikasyon bon jan kalite a, ka bay sètifika bon jan kalite, epi li sijè a tès twazyèm pati -.

 

P295GH presyon veso asye nou an ka Customized nan gwosè, koupe, soude, pwensonaj ak lòt sèvis pwosesis dapre kondisyon fen ou -itilize pou pwodwi plak asye chodyè P295GH.

 

 
Chodyè Plak ChimikKonpozisyon

 

Steel Klas C Si Mn P max S max Al N Kr Cu Mo Nb Ni Ti V
P295GH 0.08 a 0.20 Mwens pase oswa egal a 0.40 0.90crive 1.50 0.025 0.015 Mwens pase oswa egal a 0.020 Mwens pase oswa egal a 0.012d Mwens pase oswa egal a 0.30 Mwens pase oswa egal a 0.30 Mwens pase oswa egal a 0.08 Mwens pase oswa egal a 0.020 Mwens pase oswa egal a 0.30 0.03 Mwens pase oswa egal a 0.02

 

 
Chodyè presyon veso Steel Plak pwopriyete mekanik

 

Steel Klas Epesè mm Fòs Sede Mpa Pi gran pase oswa egal a Fòs rupture
Mpa
Elongasyon % Pi gran pase oswa egal a Enpak Minimòm Pouvwa Tanperati
P295GH Mwens pase oswa egal a 16 295 460-580 21 27 34 40
16<t Mwens pase oswa egal a 40 290
40<t Mwens pase oswa egal a 60 285
60<t Mwens pase oswa egal a 100 260
100<t Mwens pase oswa egal a 150 235 440-570
150<t Mwens pase oswa egal a 250 220 430-570

 

Veso presyon ak pwodwi plak chodyè imaj

 

pressure vessel steel plate

 

 
Foto ekip gwoup GNEE

 

pressure vessel plate material

 

 
Vizit kliyan gwoup GNEE

 

vessel steel plate

 

 
 
GNEE Group asye egzibisyon

 

boiler steel

 

Nou gen ekselan apre-lavant sèvis. Si ou gen nenpòt kesyon sou P295GH cho woule presyon veso asye plak, ou ka kontakte nou epi nou pral reponn ou nan de zè de tan.

 

Baj popilè: p295gh cho woule presyon veso asye plak, Lachin p295gh cho woule presyon veso asye plak manifaktirè, Swèd, faktori