Din 17155 15 MO3 pou plak veso presyon

Din 17155 15 MO3 pou plak veso presyon

15MO3 plak asye, din 17155 15 MO3 plak asye, anba DIN 17155 estanda, nou ka konsidere 15MO3 plak asye pou asye chofaj.Din estanda 15MO3 veso veso asye kounye a te ranplase ak spesifikasyon yo euro nòm en 10028. GNEE se youn nan DIN 15MO3 plak asye. Nou gen anpil eksperyans nan fabrike DIN 15MO3 plak asye. Tan nan livrezon pi rapid ak pri konpetitif ka dirèkteman ofri soti nan konpayi nou an.
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

15mo3 Steel konpozisyon chimik

Egalize C. Max Mn. S. N CU Si. P. Cr. Ni. Mo.
15mo3 0.12- 0.2 0.40- 0.90 0.01 0.012 0.30 0.35 0.025 0.30 0.30 0.25- 0.35

15MO3 Steel Propertites

Egalize Fòs rupture (MPa) Sede fòs (MPa) Elongasyon nan 100-150 mm (%) Elongasyon nan 16 mm (%) Epesè max (mm)
15mo3 440-590 220-275 19 24 250

 

 

 


1. Kijan kontni MOLYBDENUM (0.25-0.35%) pèfòmans benefis?

Repons:
Anplis de sa a MOLYBDENUM bay:
✔ Amelyore rezistans fluajnan tanperati ki wo
✔ Amelyore estabilite microstructuralanba monte bisiklèt tèmik
✔ Pi bon rezistans idwojèn embrittlement
✔ Ogmante retansyon fòsPi wo pase 400 degre


2. Ki tretman chalè ki nesesè?

Repons:
Pwosesis estanda:

Nòmalize(900-950 degre) pou tout epesè

Si ou vle tanperaman (580-680°C) for thickness >50mm

Estrès sekou rkwir(600-650 degre) pou aplikasyon kritik


3. Ki pwosedi soude yo rekòmande?

Repons:
Pratik soude kritik:

Chèz: 150-200°C (for t>15mm)

Consommables: DIN 8556 E Mo 2 0 oswa ekivalan

Chalè opinyon: 1.8-3.0 kJ/mm

Entèrpass temp: Mwens pase oswa egal a 300 degre

PWHT: Obligatwa (650-680 degre × 1hr/25mm)


4. Ki kote 15MO3 tipikman espesifye?

Repons:
Aplikasyon Prensipal:

Power Plant Chodyè Tanbou(Mwens pase oswa egal a 525 degre)

High-tanperati echanjeur chalè

Ekipman raffinage petwòl

Pwosesis sistèm kanalizasyon

Veso sèvis idwojèn


Tab konparezon

Egalize Mo kontni Max temp Estanda ekivalan
15mo3 0.25-0.35% 525 degre En 10028-2 16 Mo3
13crmo4-5 0.45-0.65% 550 degre ASTM A387 Gr.12
10crmo9-10 0.90-1.10% 600 degre ASME SA387 Gr.22

Baj popilè: DIN 17155 15 MO3 pou plak veso presyon, Lachin din 17155 15 MO3 pou manifaktirè plak veso presyon, founisè, faktori