S275M ak S275N se asye estriktirèl estanda Ewopeyen an ak yon fòs sede minimòm de 275 MPa, ki diferan sitou nan kondisyon livrezon yo: S275M (EN 10025-4) se thermomechanically woule (M) pou soudabilite ekselan, pandan y ap S275N (EN 10025{{10} ) bay garanti}}3{{10}. rezistans ba-tanperati, ak S275NL ki ofri menm pi frèt rezistans. Tou de se asye amann, men 'N' (Nòmalize) vle di pi bon duktilite ak fòs enpak nan tan ki ba, apwopriye pou pon, konstriksyon, ak enèji, kontrèman ak 'M' (TMCP) ki konsantre sou woule kontwole.
Pwopriyete mekanik pou plak asye S275N
| Epesè (mm) | ||||||||
| S275N | Mwens pase oswa egal a 16 | >16 Pi piti oswa egal a 40 | >40 Mwens oswa egal a 63 | >63 Mwens pase oswa egal a 80 | >80 Mwens pase oswa egal a 100 | >100 Mwens pase oswa egal a 150 | >150 Mwens pase oswa egal a 200 | > 200 |
| Fòs sede (pi gran pase oswa egal a Mpa) | 275 | 265 | 255 | 245 | 235 | 225 | 215 | 205 |
| Mwens pase oswa egal a 100 | >100 Mwens pase oswa egal a 200 | > 200 | ||||||
| Fòs rupture (Mpa) | 370-510 | 350-480 | 350-480 | |||||
Pwopriyete mekanik pou plak asye S275M
| Klas |
Epesè | Sede fòs | Fòs rupture | Elongasyon | Enèji enpak |
| (mm) | MPa (min) | MPa | % (min) | (KV J) (min) | |
| -20 degre | |||||
| S275M | Mwens pase oswa egal a 16 | 275 | 370-530 | 24 | 40 |
| 16>a mwens pase oswa egal a 40 | 265 | 370-530 | 24 | 40 | |
| 40>a mwens pase oswa egal a 63 | 255 | 350-510 | 24 | 40 | |
| 63>a mwens pase oswa egal a 80 | 245 | 350-510 | 24 | 40 | |
| 80>a mwens pase oswa egal a 100 | 245 | 350-510 | 24 | 40 | |
| 100>a mwens pase oswa egal a 120 | 240 | 350-510 | 24 | 40 |
Konpozisyon chimik pou plak asye S275N
| Pwensipal eleman chimik konpozisyon plak asye S275N | ||||||
| C | Si | Mn | P | S | Nb | V |
| 0.18 | 0.40 | 0.50-1.50 | 0.030 | 0.025 | 0.05 | 0.05 |
| Al(total) | Ti | Kr | Ni | Mo | Cu | N |
| Pi gran pase oswa egal a 0.02 | 0.05 | 0.30 | 0.30 | 0.10 | 0.55 | 0.015 |
Konpozisyon chimik pou plak asye S275M
| EN10025-4 S275M konpozisyon chimik | |||||||
| Klas | Eleman Max (%) | ||||||
| C | Si | Mn | P | S | Al | N | |
| S275M | 0.15 | 0.55 | 1.60 | 0.030 | 0.030 | 0.015 | |
| Nb | V | Ti | Cu | Kr | Ni | Mo | |
| 0.06 | 0.10 | 0.06 | 0.60 | 0.35 | 0.35 | 0.13 | |
S275M Steel Plak
Estanda: EN 10025-4 (Thermomechanically woule).
Kondisyon livrezon: "M" pou Thermomechanical Rolling (TMCP), lè l sèvi avèk woule kontwole ak refwadisman akselere.
Pwopriyete: Grenn byen -, soude, bon fòs.
Pi bon pou: Aplikasyon ki bezwen bon soudabilite ak fòs san yo pa bezwen separe tretman chalè nòmal.
S275N Steel Plak
Estanda: EN 10025-3 (Normalize).
Kondisyon livrezon: "N" pou nòmalize, yon pwosesis tretman chalè.
Pwopriyete: Grenn byen -, soude, ak garanti ba -tanperati solidite (egzanp, 47 Joules nan -20 degre).
S275NL: Yon varyasyon ki ofri menm pi di pèfòmans ba-tanperati (pa egzanp, 27 Joules nan -50 degre).
Pi bon pou: Anviwònman modere ak frèt, estrikti ki bezwen garanti rezistans enpak tankou pon, trepye, ak machin lou.
Diferans kle yo rezime
Pwosesis: S275M itilize TMCP (M), S275N itilize Nòmalizasyon (N).
Tès Enpak: S275N/NL gen espesifik garanti enèji enpak ba-tanperati, esansyèl pou klima frèt, yon karakteristik ki pa nannan S275M san plis pwosesis.
Konsantre aplikasyon: S275M ekselan nan fabwikasyon, pandan y ap S275N/NL ofri asire pèfòmans tanperati ba -.