SS490 is a type of high-strength, low-alloy carbon steel plate that falls under the Japanese Industrial Standards (JIS) G3101 standard. It is a versatile material used in general structural applications such as bridges, ships, and construction machinery, and it has mechanical properties including a tensile strength of 490-610 MPa and a minimum yield strength of 275 MPa.

 



Simulated post-welded heat treatment (PWHT)
Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2

Rolling under ASTM A6/A6M for Genenal requirements of structural used steel

 

SS490 steel plate Chemical analysis

 

C<= 16mm max C>16mm max
P
max.
S
max.
0.24 0.24 0.55 1.60 0.045 0.045

 

SS490 steel plate Mechanical properties

 

Yield StrengthReH[N/mm2] transv.min.

[N/mm2]transv.

Fracture Elongation[%]transv. min. Notch Impact Energy1)Ch Vcomplete samplelongitud. min [J]
t≤ 16mm t >16mm 355 345     20℃27J
t < 3mm t >= 3mm   510-680 490-630  
Up to 1.5mm 1.51-2.00mm 2.01-2.50mm 2.51-2.99mm >= 3mm     13 14 15 16 20

 

Other applications: Railway equipment and other structural components.