A516 GR60 plak asyese pou plak veso presyon, asye kabòn pou sèvis tanperati modere ak ba soti nan US spesifikasyon ASTM A516 / SA516M. Konsidere objektif presyon ak fòs sede ak pwopriyete mekanik valè minimòm, Nan spesifikasyon estanda BS EN 10028-2 P265GH asye plak ekivalan a ASTM A516 GR60 plak asye.
GNEE kap founi ASTM A516 GR60 plak asye ak plak asye P265GH soti nan tou de stock ak woule plan.Standard dimansyon pou A516 GR60 asye plak kòm 2000 * 6000mm, 2438 * 9144mm, 2200 * 10000mm, 2500 * 10000mm * 10000mm dwe teste 1219. emèt ak fòma kòm estanda EN 10204 3.1/3.2 oswa ISO 10474 3.1/3.2 oswa DIN 50049 3.1/3.2.
|
A516 GR60vsP265GH |
Konpozisyon chimik: analiz chalè Max% |
|||||||||
|
Estanda |
Klas |
C |
Mn |
P |
S |
Si |
N |
Alt min. |
Kr |
Cu |
|
ASTM A516/A516M |
A516 GR60 |
0.21 |
0.6-0.9 |
0.035 |
0.035 |
0.15-0.40 |
- |
- |
- |
- |
|
EN 10028-2 |
P265GH |
0.20 |
0.8-1.5 |
0.025 |
0.010 |
0.40 |
0.012 |
0.02 |
0.30 |
0.30 |
|
Pwopriyete mekanik: |
Epesè |
Sede fòs |
Fòs rupture |
|||||||
|
Mpa Min. |
Mpa |
|||||||||
|
ASTM A516/A516M |
A516 GR60 |
|
220 |
415-550 |
||||||
|
EN 10028-2 |
P265GH |
T Mwens pase oswa egal a 16 |
265 |
410-530 |
||||||
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis pase kontan ede w.
Ki sa en 10028-2 P265GH ekivalan a?
ASTM A516 GR60 asye
Lè ou konsidere objektif presyon ak fòs sede ak valè minimòm pwopriyete mekanik, nan spesifikasyon estanda BS EN 10028-2 P265GH plak asye ekivalan aASTM A516 GR60 plak asye.
Ki klas materyèl P265GH?
P265GH klas se aestanda veso presyon soude ak klas asye chodyè. TheP265GH Plate a fèt ak yon kontni chimik ekselan bay li bon pèfòmans nan diferan anviwònman. P265gh Steel Plateis ideyal pou itilize nan sèvis tanperati ki wo, ki komen nan endistri pétrochimique ak chimik.
Ki sa ki materyèl A516 gr 60?
kabòn-asye Manganèz
Pwodwi plak asye SSAB A516-60 ak ASME SA516-60 yo te fè soti nankabòn-asye Manganèzak pwodwi nan estanda kalite veso presyon (PVQ) jan sa endike nan ASTM A20 / ASME SA20.
Ki diferans ki genyen ant A36 ak A516 gr 60?
A36 se yon klas asye kabòn jeneral -ki apwopriye pou aplikasyon estriktirèl, pandan y ap A516 fèt espesyalman pou aplikasyon pou veso presyon epi li ofri rezistans siperyè.
Ki ranje tanperati yon 516 GR 60?
Sa 516 Gr 60 devlope pou aplikasyon pou tanperati ki ba -. Modil sa yo ka opere nan tanperatiosi ba ke -45 degre Sèlsiyis epi li ka andire tanperati ki wo tankou 340 degre.



| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Klas3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||