A516 Steel Plak gwosè ki disponib
Gnee Steel stock gwosè estanda sa yo nan lokal Entènasyonal, men lòt gwosè ka disponib pou lòd espesyal.
| KLAS | Epesè | LAJÈ | LONGÈ |
| 55 | 3/16" – 8" | 48" – 120" | Jiska 480" |
| 60 | 3/16" – 8" | 48" – 120" | Jiska 480" |
| 65 | 3/16" – 8" | 48" – 120" | Jiska 480" |
| 70 | 3/16" – 8" | 48" – 120" | Jiska 480" |
Pwopriyete mekanik pou plak asye SA516 Gr55:
| Fòs sede (Mpa) | Fòs rupture (Mpa) | Elongasyon nan pi gran pase oswa egal a,% | |
| 205 | 380-515 | 200mm | 50mm |
| 23 | 27 | ||
Konpozisyon chimik pou plak asye SA516 Gr55 (Analiz pwodwi Max%)
| Pwensipal eleman chimik konpozisyon SA516 Gr55 | |||||
| Epesè (mm) | C | Si | Mn | P | S |
| T Mwens pase oswa egal a 12.5 | 0.18 | 0.13-0.45 | 0.55-0.98 | 0.035 | 0.035 |
| 12.5<> | 0.20 | 0.55-1.30 | |||
| 50<> | 0.22 | ||||
| 100<> | 0.24 | ||||
| T>200 | 0.26 | ||||