S355J2G2W plak asye

Nov 20, 2025 Kite yon mesaj

Fèy asye S355J2G2W, plak asye EN S355J2G2W, plak asye S355J2G2W, anba estanda EN 10155, nou ka konsidere plak asye S355 J2G2W kòm Steel rezistan a korozyon atmosferik. Plak asye S355 J2G2W se youn sitou nan asye rezistan a korozyon atmosferik, plak asye S355J2G2W a reprezante kalite debaz nan asye estriktirèl ki souvan itilize sèjousi. Fòs minimòm sede li se 355MPa.

 

Konpozisyon chimik % analiz pwodwi S355J2G2W

 

Klas

C%

Si%

Mn%

P%

S%

Cr%

Cu%

S355J2G2W

0.16

0.50

0.50-1.50

0.035

0.035

0.40-0.80

0.25-0.55

 

Pwopriyete mekanik nan klas S355J2G2W:

 

Klas

Epesè (mm)

Sede Minim (MPa)

Tensile (MPa)

Elongasyon

Min (%)

Tès

Tanperati (degre

 

S355J2G2W

5<t Mwens pase oswa egal a 16

355

490-630

22

 

 

S355J2G2W

16<t Mwens pase oswa egal a 40

345

490-630

22

 

 

S355J2G2W

40<t Mwens pase oswa egal a 63

335

490-630

21

 

 

S355J2G2W

63<t Mwens pase oswa egal a 80

325

490-630

20

 

 

S355J2G2W

80<t Mwens pase oswa egal a 100

315

490-630

20

 

 

 

 

Klas

 

S235

J0W

S235

J2W

S355

J0WP

S355

J2WP

S355

J0W

S355

J2G1W

S355

J2G2W

S355

K2G1W

S366

K2G2W

Tès

Tanperati (degre)

0

-20

0

-20

0

-20

-20

-20

-20