P500QL1 plak asye

Sep 19, 2025 Kite yon mesaj

EN10028-6 P500QL1 Creole Specification Forweldable Fine Steels grenn Fine, pasè ak apeze .P500QL1 klas gen yon bon soude ak itilize nan ekipman tanperati ki wo ak veso presyon.

 

P500QL1 konpozisyon chimik

Egalize

Eleman max la (%)

C

Si

Mn

P

S

N

B

P500QL1

0.18

0.60

1.70

0.020

0.010

0.015

0.005

Mwa

CU

NB

NI

Ti

V

Cr

0.70

0.3

0.05

1.50

0.05

0.08

1.00

Kabòn ekivalan: CEQ=【C+Mn/6+ (Cr+Mo+V)/5+ (Ni+Cu)/15】%

 

 

Egalize

 

P500QL1 pwopriyete mekanik

Epesè

Rekòlt

Raman

Elongasyon

P500QL1

mm

Min MPA

MPA

Min %

6-50

500

590-770

17%

50-100

480

590-770

17%

100-150

440

540-720

17%

 

EN10028-6 P500QL1 veso presyon ak aplikasyon asye plak chodyè

EN10028-6 P500QL1 veso presyon ak plak asye chodyè yo te itilize nan veso presyon, chofaj, tank depo ak echanjeur chalè nan lwil oliv, pwojè gaz.

 

EN10028-6 P500QL1 veso presyon ak plak asye chodyè Lòt non

EN10028-6 P500QL1 Chodyè Steel Plak|EN10028-6 P500QL1 Presyon Veso Steel Plak|EN10028-6 P500QL1 Depo tank Steel Plak |

 

Lòt kondisyon

UT (egzamen ultrasons), AR (tankou cho woule sèlman), TMCP (tèmik pwosesis kontwòl mekanik), N (normalized), Q+T (pasè ak apeze), z tès direksyon (Z15, Z25, Z35), Charpy V - tès enpak, tankou SG.