P500 QL2 Steel Plak

Sep 19, 2025 Kite yon mesaj

EN10028-6 P500QL2, EN 10028-6 P500 QL2 Steel Plak EN10028-6 P500QL2 Creole Specification Forweldable Fine grenn asye, janm pase ak apeze. Klas P500QL2 gen yon bon soudab ak itilize nan ekipman tanperati ki wo ak veso presyon.

 

Epesè: 6mm a 300mm,

Lajè: 1500mm a 4050mm,

Longè: 3000mm a 15000mm

 

P500QL2 konpozisyon chimik

Egalize

Eleman max la (%)

C

Si

Mn

P

S

N

B

P500QL2

0.18

0.60

1.70

0.020

0.010

0.015

0.005

Mwa

CU

NB

NI

Ti

V

Cr

0.70

0.3

0.05

1.50

0.05

0.08

1.00

Kabòn ekivalan: CEQ=【C+Mn/6+ (Cr+Mo+V)/5+ (Ni+Cu)/15】%

 

 

Egalize

 

P500QL2 pwopriyete mekanik

Epesè

Rekòlt

Raman

Elongasyon

P500QL2

mm

Min MPA

MPA

Min %

6-50

500

590-770

17%

50-100

480

590-770

17%

100-150

440

540-720

17%

 

EN10028-6 P500QL2 veso presyon ak aplikasyon asye plak chodyè

EN10028-6 P500QL2 veso presyon ak plak asye chodyè yo te itilize nan veso presyon, chofaj, tank depo ak echanjeur chalè nan lwil oliv, pwojè gaz.

 

EN10028-6 P500QL2 veso presyon ak plak asye chodyè Lòt non

EN10028-6 P500QL2 Plak Steel Chodyè|EN10028-6 P500QL2 Presyon Veso Steel Plak|EN10028-6 P500QL2 Tank Plak Steel |

 

Lòt kondisyon

UT (egzamen ultrasons), AR (tankou cho woule sèlman), TMCP (tèmik pwosesis kontwòl mekanik), N (normalized), Q+T (pasè ak apeze), z tès direksyon (Z15, Z25, Z35), Charpy V - tès enpak, tankou SG.