LR DH32 konstriksyon bato aplikasyon asye
LR DH32 asye plak/fèy yo itilize pou konstriksyon bato ak objektif platfòm lwil oliv ak yo apwouve pa ABS, DNV, GL, BV, LR, NK, RINA ak lòt sosyete klasifikasyon. Ki sa ki nan plis, Dh32 konstriksyon bato plak ka itilize nan fabrikasyon estrikti ekòs bato a ki gen pwa ki anba a 10000 tòn.
LR DH32 konstriksyon bato gwosè ekipman pou
Epesè: 4mm-260mm
Lajè: 1200mm-4000mm
Longè: 3000mm-18000mm
(Lòt gwosè plak ak epesè ki disponib sou demann)
|
LR/DH32 segondè fòs konpozisyon chimik |
|||||||
|
Egalize |
Eleman max la (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
LR/DH32 |
0.18 |
0.05 |
0.9-1.6 |
0.035 |
0.035 |
0.015 |
|
|
NB |
V |
Ti |
CU |
Cr |
NI |
Mwa |
|
|
0.02-0.05 |
0.03-0.10 |
0.02 |
0.35 |
0.20 |
0.40 |
0.08 |
|
|
LR/DH32 segondè pwopriyete fòs |
|||||||
|
Egalize |
|
Pwopriyete mekanik |
Charpy V tès enpak |
||||
|
Epesè |
Rekòlt |
Raman |
Elongasyon |
Degre |
Enèji 1 |
Enèji 2 |
|
|
LR/DH32 |
mm |
Min MPA |
MPA |
Min |
-20 |
J |
J |
|
t mwens pase oswa egal a 50 |
315 |
440-590 |
22% |
20 |
31 |
||
|
50 < T mwens pase oswa egal a 70 |
315 |
440-590 |
22% |
26 |
38 |
||
|
70 < T mwens pase oswa egal a 100 |
315 |
440-590 |
22% |
31 |
46 |
||
|
Remak: enèji 1 se tès enpak Transverse, enèji 2 se Longitudinal |
|||||||
|
Ekivalan asye klas nan LR/DH32 |
|||||||
|
Dnv |
Gl |
Ab |
Ji |
CCS |
Nk |
Kr |
Kòn |
|
NV D32 |
Gl - D32 |
AB/DH32 |
BV/DH32 |
CCS/DH32 |
K D32 |
R D32 |
RI/D32I/D32 |
Klas ki gen rapò: LR/AH32|LR/EH32|LR/FH32
|
LR Steel Plak Klas Founisè |
||||
|
Fòs jeneral |
LR/A |
LR/B |
LR/D |
LR/E |
|
Gwo fòs |
LR/AH32 |
LR/DH32 |
LR/EH32 |
LR/FH32 |
|
LR/AH36 |
LR/DH36 |
LR/EH36 |
LR/FH36 |
|
|
LR/AH40 |
LR/DH40 |
LR/EH40 |
LR/FH40 |
|
|
Fòs siplemantè |
LR/AH42 |
LR/DH42 |
LR/EH42 |
LR/FH42 |
|
LR/AH46 |
LR/DH46 |
LR/EH46 |
LR/FH46 |
|
|
LR/AH50 |
LR/DH50 |
LR/EH50 |
LR/FH50 |
|
|
LR/AH55 |
LR/DH55 |
LR/EH55 |
LR/FH55 |
|
|
LR/AH62 |
LR/DH62 |
LR/EH62 |
LR/FH62 |
|
|
LR/AH69 |
LR/DH69 |
LR/EH69 |
LR/FH69 |
|