Offshore ak Marin Steel Plak

Offshore ak Marin Steel Plak

Pwodwi: Offshore ak Marin Steel Plak
Kalite: plak asye
Estanda: EN10225 API
Tolerans: ± 1%
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

Offshore ak Marin Steel Plak


Plak asye platfòm lanmè yo se plak asye yo itilize nan konstriksyon platfòm lwil oliv ak platfòm perçage. Nou kapab bay divès kalite plak asye platfòm lanmè. Nou ka satisfè estanda tankou EN10225, API, BS 7191 ak ASTM. Plak asye platfòm lanmè nou yo te pase tès sa yo: tès enpak tanperati ki ba ak tès enpak Charpy V-dan. Nou menm tou nou bay piki eksplozif ak penti, koupe ak soude sèvis selon kondisyon itilizatè a fen.

 

 
Klas Steel ki disponib pou Plak platfòm Offshore

 

Adopte Estanda

Steel Klas

EN 10225

S355G2+N, S355G5+M, S355G3+N, S355G6+M, S355G7+N, S355G7+M, S355G8+M, S355G8+N, S355G9+N, S355G9+M, S355G10+N, S355G10+M, S420G1+Q, S420G2+Q, S460G1+Q, S460G2+Q

API

API 2H Gr50, API 2W Gr50, API 2W Gr50T, API 2W Gr60, API 2Y Gr60

BS 7191

355D, 355E, 355EM, 355EMZ, 450D, 450E, 450EM, 450EMZ

ASTM A131/A131M

A131 Klas A, A131 Klas B, A131 Klas D, A131 Klas E, A131 Klas AH32, A131 Klas AH36, A131 Klas AH40, A131 Klas DH32, A131 Klas DH36, A131 Klas AH31 DH41, Klas E EH36, A131 Klas EH40, A131 Gr FH32, A131 Gr FH36, A131 Gr FH40

 

 
EN10225 estanda estriktirèl asye plak konpozisyon chimik

 

Konpozisyon prensipal eleman chimik S355G3+N

C

Si

Mn

P

S

Kr

Mo

0.18

0.50

0.90-1.65

0.030

0.025

0.30

0.10

Ni

Alt min.

Cu

N

Nb

Ti

V

0.50

0.020

0.35

0.015

0.060

0.030

0.12

 

Konpozisyon prensipal eleman chimik S355G5+M

C

Si

Mn

P

S

Kr

Mo

0.14

0.50

1.60

0.035

0.030

-

0.20

Ni

Alt min.

Cu

N

Nb

Ti

V

0.30

0.020

-

0.015

0.050

0.050

0.10

 

 

C max.

Si

Mn

S

max.

P

max.

Kr

max.

Mo

max.

Nb

max.

V

max.

Ti

max.

Ni

max.

Cu

max.

Al(tot)

N

max.

S355G8+M

S355G8+N

0.14

0.15
/0.55

1.00
/1.65

0.007

0.02

0.25

0.08

0.04

0.06

0.025

0.5

0.3

0.015
/0.055

0.01

 

Klas

Konpozisyon chimik (%)

C

Mn Max

Si Max

P

S

S355G10+M

0.12

1.65

0.15-0.55

0.015

0.005

 

 
EN10225 estanda Offshore Steel Plak dimansyon

 

Klas Minimòm epesè (mm) Maksimòm epesè (mm)
S355G2+N 5 20
S355G3+N 40
S355G5+M 20
S355G6+M 40
S355G7+N 80
S355G7+M 50
S355G8+N 80
S355G8+M 50
S355G9+N 80
S355G9+M 50
S355G10+N 80
S355G10+M 50
S420G1+M 30
S420G2+M

 

 
Offshore Platfòm Steel Plak Pwodwi imaj

 

China offshore structural steel Suppliers

 

 
Foto ekip gwoup GNEE

 

China offshore steel Suppliers

 

 
Vizit kliyan gwoup GNEE

 

China offshore steel plate Distributors

 

 
Gwoup GNEE patisipe nan ekspozisyon asye etranje yo

 

offshore structural steel plates