316 Nerjaveèi Round Bar
316 se estanda Ameriken an anba klas la, ki dwe nan asye pur, chalè -rezistan, korozyon-rezistan, se asye pur austenitic. Pou estanda nasyonal la se 0Cr17Ni12Mo2. se pi bon pase 304 asye pur. Nan dlo lanmè ak lòt medya. Rezistans korozyon pi bon pase 0Cr19Ni9.
316 Nerjaveèi asye: 316 Nerjaveèi gen molybdène ak kontni kabòn ki ba, nan oseyan an ak anviwònman endistri chimik nan rezistans nan korozyon pitting se anpil siperyè pase 304 asye pur! (316L ba kabòn, 316N ki gen nitwojèn gwo fòs, 316 asye pur ki gen gwo souf, fasil koupe asye pur).
316 wonn konpozisyon chimik asye
| Kabòn (C) | Manganèz (Mn) | Fosfò (P) | Souf (S) | Silisyòm (Si) | Chrome (Cr) | Nikèl (Ni) | Molybdène (Mo) | |
|---|---|---|---|---|---|---|---|---|
| Min | 16.0 | 10.0 | 2.00 | |||||
| Max | 0.030 | 2.00 | 0.045 | 0.030 | 1.00 | 18.0 | 14.0 | 3.00 |
316 asye wonn pwopriyete mekanik
| Tensile Min psi | Sede Min psi | Elongasyon Min% | Rediksyon Min% | Dite BHN |
|---|---|---|---|---|
| 75,000 | 30,000 | 40 | 50 | * |
316 gwosè aksyon wonn asye
| Dia (mm) |
Pwa pou chak mèt (kg) | Dia (nan) | Pwa pou chak mèt (kg) | |
|---|---|---|---|---|
| 3mm | 0.06 | 1/8" | 0.06 | |
| 4mm | 0.10 | 3/16" | 0.14 | |
| 5mm | 0.16 | 1/4 | 0.25 | |
| 6mm | 0.23 | 5/16" | 0.39 | |
| 8mm | 0.40 | 3/8 | 0.57 | |
| 10mm, | 0.63 | 7/16" | 0.77 | |
| 12mm | 0.90 | 1/2 | 1.01 | |
| 14mm | 1.23 | 9/16" | 1.28 | |
| 15mm | 1.41 | 5/8" | 1.58 | |
| 16mm | 1.60 | 11/16 | 1.91 | |
| 18mm | 2.03 | 3/4" | 2.27 | |
| 20mm | 2.50 | 7/8 | 3.09 | |
| 24mm | 3.60 | 1" | 4.03 | |
| 25mm | 3.91 |
| Gwosè (mm) | Pwa pou chak mèt (kg) | Gwosè (mm) | Pwa pou chak mèt (kg) |
|---|---|---|---|
| 20x10 | 1.58 | 50 x 15 | 5.93 |
| 25x10 | 1.98 | 60 x 15 | 7.11 |
| 30 x 10 | 2.37 | 75 x 15 | 8.88 |
| 40x10 | 3.16 | 100 x 15 | 11.90 |
| 50 x 10 | 3.95 | 25 x 20 | 3.95 |
| 60 x 10 | 4.74 | 30 x 20 | 4.74 |
| 75 x 10 | 5.93 | 40 x 20 | 6.32 |
| 100 x 10 | 7.90 | 50 x 20 | 7.90 |
| 25 x 12 | 2.37 | 60 x 20 | 9.48 |
| 30 x 12 | 2.84 | 75 x 20 | 11.90 |
| 40 x 12 | 3.79 | 100 x 20 | 15.80 |
| 50 x 12 | 4.74 | 30 x 25 | 5.93 |
| 60 x 12 | 5.69 | 40 x 25 | 7.90 |
| 75 x 12 | 7.11 | 50 x 25 | 9.88 |
| 100 x 12 | 9.48 | 60 x 25 | 11.90 |
| 25 x 15 | 2.96 | 75 x 25 | 14.80 |
| 30 x 15 | 3.56 | 100 x 25 | 19.80 |
| 40 x 15 | 4.74 |
Pi wo a se kèk enfòmasyon gwosè estanda!
Tanpri kontakte nou pou plis enfòmasyon estanda gwosè!
Poukisa chwazi nou?
1. Pri konpetitif ak bon jan kalite soti nan faktori pwòp nou yo
2. Apwouve pa ISO9001, CE, SGS chak ane
3. Pi bon sèvis ak repons 24 èdtan
4. peman fleksib ak T/T, Paypal, elatriye
5. Lis pwodiksyon kapasite (50000tons / mwa)
6. Livrezon rapid ak pake ekspòte estanda
7. OEM/ODM
Nerjaveèi asye wonn pwodwi imaj

Foto ekip gwoup GNEE

Vizit kliyan gwoup GNEE


Nou gen ase envantè epi nou ka pake ak bato nan tan ki pi kout la. Si ou gen bezwen pou 316 Nerjaveèi Round Bar oswa lòt pwodwi metal wonn stock, tanpri kontakte m '.
Baj popilè: 316 Nerjaveèi wonn bar, Lachin 316 Nerjaveèi wonn ba manifaktirè, Swèd, faktori