GB/T713 Low Alloy Presyon Veso Plak
GB/T 713 se estanda nasyonal Chinwa a pou plak asye pou veso presyon. Estanda sa a espesifye sa ki nan lòd la nan plak asye pou chodyèr ak veso presyon, ekspresyon an nan klas, dimansyon, fòm, pwa ak devyasyon akseptab, kondisyon teknik, metòd tès, règ enspeksyon, anbalaj, make ak bon jan kalite sètifika ak sou sa.
Klas nou ka bay pou estanda GB yo ye
|
GB |
GB713Q245R,Q345R,Q370R,18MnMoNbR,13MnNiMoR, 15CrMoR, 14Cr1MoR, 12Cr2Mo1R, 12Cr1MoVR GB3531 16MnDR,15MnNiDR,09MnNiDR elatriye |
q245R veso plak konpozisyon chimik
| C | Si | Mn | P | S | Al |
| 0.20 max. | 0.35 max. | 0.50-1.00 | 0.025 max. | 0.015 max. | 0.020 min. |
Q345R chodyè plak konpozisyon chimik
| Klas |
C% |
SI% |
Mn% |
Cr% |
Ni% |
Mo% |
Nb% |
V% |
P% |
S% |
Alt% |
|
Q345R |
Mwens pase oswa egal a O.20 |
Mwens pase oswa egal a 0.55 |
1.20-1.60 |
|
|
|
|
Mwens pase oswa egal a 0.025 |
Mwens pase oswa egal a 0.015 |
Pi gran pase oswa egal a 0.020 |
|
Q370R chodyè asye plak konpozisyon chimik
| Klas | C% | SI% | Mn% | Cr% | Ni% | Mo% | Nb% | V% | P% | S% | Alt% |
| Q370R | Mwens pase oswa egal a O.18 | Mwens pase oswa egal a 0.55 | 1.20-1.60 | 0.015-0.050 | Mwens pase oswa egal a 0.025 | Mwens pase oswa egal a 0.015 | |||||
18MnMoNbR asye chodyè plak konpozisyon chimik
| Klas | C% | SI% | Mn% | Cr% | Ni% | Mo% | Nb% | V% | P% | S% | Alt% |
| 18MnMoNbR | Mwens pase oswa egal a O.22 | 0.15-0.50 | 1.20-1.60 | 0.45-0.65 | 0.025-0.050 | Mwens pase oswa egal a 0.020 | Mwens pase oswa egal a 0.010 | ||||
13MnNiMoR chodyè plak asye konpozisyon chimik
| C | Si | Mn | Kr | Ni | Mo | Nb | P | S |
| Mwens pase oswa egal a 0.15 | 0.15-0.50 | 1.20-1.60 | 0.20-0.40 | 0.60-1.00 | 0.20-0.40 | 0.005-0.020 | Mwens pase oswa egal a 0.020 | Mwens pase oswa egal a 0.010 |
15CrMoR presyon veso plak konpozisyon chimik
|
C |
Si |
Mn |
P |
S |
Kr |
Mo |
|
0.12-0.18 |
0.15-0.40 |
0.40-0.70 |
Mwens pase oswa egal a 0.025 |
Mwens pase oswa egal a 0.010 |
0.80-1.20 |
0.3-0.60 |
14Cr1MoR presyon veso asye plak konpozisyon chimik
|
C |
Si |
Mn |
P |
Kr |
Mo |
Ni |
|
0.05%-0.17% |
0.50%-0.80% |
0.40%-0.65% |
0.010%-0.012% |
1%-1.5% |
0.45%-0.65% |
0.20%-0.25% |
12Cr2Mo1R presyon veso plak materyèl konpozisyon chimik
| C | Si | Mn | P | S | Kr | Mo |
| 0.08-0.15 | 0.50 | 0.30-0.60 | 0.020 | 0.010 | 2.00-2.50 | 0.90-1.10 |
12Cr1MoVR veso asye plak konpozisyon chimik
| Klas | C | Si | Mn | Cu | Ni | Kr | Mo | Nb | V | Ti | Alt | P | S |
| 12Cr1MoVR | 0.08-0.15 | 0.15-0.40 | 0.40-0.70 | Mwens pase oswa egal a 0.30 | Mwens pase oswa egal a 0.30 | 0.90-1.20 | 0.25-0.35 | - | 0.15-0.30 | - | - | Mwens pase oswa egal a 0.025 | Mwens pase oswa egal a 0.010 |
Poukisa chwazi nou?
1. gratis echantiyon.
2. Rich mache pwevwa konsèy.
3. Repons Alè.
4. Fèmen pri pou ede ou ekonomize pri, asirans komès.
5. Liy pwodiksyon avanse, fò kapasite pwodiktif.
6. Sistèm lòd pwofesyonèl, operasyon konplè.
GB/T713 presyon veso bon jan kalite asye plak Pwodwi imaj

Foto ekip gwoup GNEE

Vizit kliyan gwoup GNEE

Gwoup GNEE patisipe nan ekspozisyon asye etranje yo

Nou gen anplwaye pwofesyonèl pou bay repons detaye sou lòd ou yo. Si w gen nenpòt kesyon sou GB/T713 Low Alloy Pressure Vessel Plate, tanpri kontakte m.