12Cr2Mo1R Presyon Veso Plak

12Cr2Mo1R Presyon Veso Plak

Kalite: plak chofaj
Estanda: AISI, ASTM, DIN, JIS, GB
Teknik: Woule cho
Fòm: Plak
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

Plak veso presyon 12Cr2Mo1R


 

Plak veso 12Cr2Mo1R fè pati chodyè alyaj ak presyon veso asye plak, 12Cr2Mo1R chodyè plak Egzekitif Creole: GB713-2014.

 

Karakteristik 12Cr2Mo1R presyon veso asye
Rezistans korozyon: 12Cr2Mo1R chodyè asye plak gen eleman chromium ak molybdène, ki gen bon rezistans korozyon epi li ka reziste ewozyon nan plizyè kalite medya chimik.


Bon pèfòmans soude: 12Cr2Mo1R asye chodyè plak se pa fasil yo pwodwi fant ak porosite pandan soude, ak jwenti yo soude gen gwo fòs, ki ka satisfè kondisyon yo soude nan veso presyon.

 

 
Chodyè Kalite Steel Plak ChimikKonpozisyon

 

Klas C% SI% Mn% Cr% Ni% Mo% V% P% S% Alt%
12Cr2Mo1R 0.08-0.15 Mwens pase oswa egal a 0.50 0.30-0.60 2.00-2.50 0.90-1.10 - Mwens pase oswa egal a 0.020 Mwens pase oswa egal a 0.010 -

 

Cho woule chodyè asye plak pwopriyete mekanik

 

Steel Klas Epesè, nan mm Fòs rupture Sede fòs, min Elongasyon, %, min
12Cr2Mo1R 6<> 520-680 310 19

 

Plak klas chodyè pwodwi imaj

 

pressure vessel steel

 

 
Foto ekip gwoup GNEE

 

boiler steel plate

 

 
Vizit kliyan gwoup GNEE

 

steel boiler plate

 

 
 
GNEE Group asye egzibisyon

 

Boiler Plate Steel

 

Nou gen ekselan apre-lavant sèvis. Si ou gen nenpòt kesyon sou plak veso presyon 12Cr2Mo1R, ou ka kontakte nou epi nou pral reponn ou nan de zè de tan.

 

Baj popilè: 12cr2mo1r presyon veso plak, Lachin 12cr2mo1r presyon veso plak manifaktirè, Swèd, faktori