P460ML1 Chodyè Steel Plak Metal
P460ML1presyon veso asye plakse yon materyèl asye pou chodyèr ak veso presyon. P460ML1plak chofajkarakterize pa yon fòs sede minimòm de 430-460 MPa ak bon soudabilite, se konsa P460ML1veso asyese sitou itilize nan fabrike chodyèr.
GNEE bay sèvis teknik adisyonèl pou P460ML1chodyè asye plak, ki gen ladan tretman chalè (nòmalizasyon, TMCP, trempe ak tanperaman, N + T), tès Z (Z15, Z25, Z35), tès ultrasons, tès enpak tanperati ki ba, DWTT, PWHT, ak koupe ak soude an moso espesyal pou itilizatè fen.
P460ML1 asye chodyè plak konpozisyon chimik
| Pwopriyete | Valè | Kondisyon | Estanda ki gen rapò | Fòm |
|---|---|---|---|---|
|
Aliminyòm |
0.02 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Kabòn |
0.16 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Manganèz |
1.7 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Molybdène |
0.2 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Nikèl |
0.5 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Niobyòm |
0.05 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Azòt |
0.02 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Fosfò |
0.02 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Silisyòm |
0.6 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Souf |
0.008 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
0.015 % |
thermomechanically woule |
EN 10028-5 |
Plak | |
|
Titàn |
0.05 % |
thermomechanically woule |
EN 10028-5 |
Plak |
|
Vanadyòm |
0.1 % |
thermomechanically woule |
EN 10028-5 |
Plak |
P460ML1 presyon veso plak pwopriyete mekanik
| Pwopriyete | Tanperati | Valè | Kondisyon | Estanda ki gen rapò | Fòm | Kòmantè |
|---|---|---|---|---|---|---|
|
Modil elastik |
190 - 210 GPa |
Tipik pou Steel |
||||
|
Elongasyon |
13.4 % |
Valè Prevwa, A200 |
||||
|
15.2 % |
Valè Prevwa, A80 |
|||||
|
17.6 % |
Valè Prevwa, Transverse |
|||||
|
18.9 % |
Prevwa Valè, A80 Transverse |
|||||
|
20.4 % |
Valè Prevwa, A5 |
|||||
|
22.2 % |
Valè Prevwa, A50 |
|||||
|
20 degre |
17 % |
thermomechanically woule |
EN 10028-5 |
Flat |
||
|
Rapò Poisson a |
0.3 [-] |
Tipik pou Steel |
||||
|
Rediksyon nan zòn nan |
39.5 % |
Valè Prevwa |
||||
|
44.2 % |
Valè Prevwa, Transverse |
|||||
|
Chea modil |
79.7 GPa |
Valè Prevwa |
||||
|
Chea fòs |
558.2 MPa |
Valè Prevwa |
||||
|
Fòs rupture |
20 degre |
530 - 720 MPa |
thermomechanically woule |
EN 10028-5 |
Flat |
|
|
Sede fòs |
261.9 MPa |
Valè Prevwa, RP1 |
||||
|
318.9 MPa |
Prevwa Valè, RP1 Transverse |
|||||
|
429.2 MPa |
Prevwa Valè, RP02 |
|||||
|
439.3 MPa |
Valè Prevwa, Transverse |
|||||
|
461.3 MPa |
Prevwa Valè, RP02 Transverse |
|||||
|
524.6 MPa |
Valè Prevwa, RP05 |
|||||
|
526.6 MPa |
Valè Prevwa, RP002 |
|||||
|
20 degre |
430 MPa |
thermomechanically woule |
EN 10028-5 |
Flat |
||
|
20 degre |
440 MPa |
thermomechanically woule |
EN 10028-5 |
Flat |
||
|
20 degre |
460 MPa |
thermomechanically woule |
EN 10028-5 |
Flat |
P460ML1 veso asye plak pwopriyete tèmik
| Pwopriyete | Valè | Kòmantè |
|---|---|---|
|
Koefisyan ekspansyon tèmik |
11.72 1/K |
Valè Prevwa |
|
Kapasite chalè espesifik |
453.7 J/(kg·K) |
Valè Prevwa |
|
Konduktivite tèmik |
37.86 W/(m·K) |
Valè Prevwa |
P460ML1 presyon veso bon jan kalite asye pwopriyete elektrik
| Pwopriyete | Valè | Kòmantè |
|---|---|---|
|
Kondiktivite elektrik |
7 S/m |
Valè Prevwa |
|
Rezistivite elektrik |
33 Ω·m |
Valè Prevwa |
chodyè bon jan kalite plak Pwodwi imaj



Foto ekip gwoup GNEE

Vizit kliyan gwoup GNEE






GNEE Group asye egzibisyon






Nou gen anplwaye pwofesyonèl sèvis sou entènèt. Si w gen nenpòt kesyon sou P460ML1 Boiler Steel Plak Metal, tanpri voye nou yon ankèt epi nou pral reponn ou nan yon jou travay.
Baj popilè: p460ml1 chodyè asye plak metal, Lachin p460ml1 chodyè asye plak metal manifaktirè, Swèd, faktori