Plak asye p355m se yon kalite materyèl pou chofaj ak veso presyon asye.
Voye rechèch
Chat kounye a
Dekri teren
Karakteristik teknik

P355m chofaj veso veso asye


P355M Plak asye chodyèKonfòme ak estanda EN10028-5. P355mplak asye vesose yon asye grenn amann grenn, anjeneral lage nan kondisyon tèmomekanik woule, ak yon fòs sede minimòm nan 355 MPa.

 

P355M Plak chofajgen bon weldability ak ekselan severite Notch, epi li se lajman itilize pa chofaj endistriyèl ak manifaktirè veso presyon ki bay sipò manifakti pou lwil oliv, gaz, endistri pétrochimik, elatriye.

 

 
P355m asye chodyè plak konpozisyon chimik

 

Eleman Min Max
(CEV) - 0.4000
(CEV) - 0.3900
(CEV) - 0.3900
(CR+Cu+MO) - 0.6000
Vanadyòm (V) - 0.1000
Titàn (TI) - 0.0500
Nikèl (Ni) - 0.5000
Niobium (NB) - 0.0500
Molibden (MO) - 0.2000
Azòt (N) - 0.0150
Aliminyòm (AL) 0.0200 -
Souf (yo) - 0.0100
Fosfò (P) - 0.0250
Manganèz (MN) - 1.6000
Silisyòm (SI) - 0.5000
Kabòn (C) - 0.1400

 

 
P355m presyon veso plak pwopriyete mekanik

 

Posesyon Tanperati Valè Kondisyon Estanda ki gen rapò Fòm Kòmante

Modil elastik

 

190 - 210 GPA

     

Tipik pou asye

Elongasyon

 

17.3 %

     

Prevwa valè, A200

   

18.4 %

     

Prevwa valè, A80

   

20.4 %

     

Valè prevwa, A80 Transverse

   

21.1 %

     

Prevwa valè, A5

   

21.4 %

     

Prevwa valè, Transverse

   

22.5 %

     

Prevwa valè, A50

 

20 degre

22 %

thermomekanikman woule

EN 10028-5

Apatman

 

Fòs rupture

20 degre

450 - 610 MPA

thermomekanikman woule

EN 10028-5

Apatman

 

Sede fòs

 

254.6 MPa

     

Valè prevwa, RP1

   

318.5 MPa

     

Valè prevwa, RP1 Transverse

   

359.6 MPa

     

Valè prevwa, RP02

   

393.3 MPa

     

Prevwa valè, Transverse

   

454.5 MPa

     

Valè prevwa, RP02 Transverse

   

468.2 MPa

     

Valè prevwa, RP05

   

493.5 MPa

     

Valè prevwa, RP002

 

20 degre

345 MPa

thermomekanikman woule

EN 10028-5

Apatman

 
 

20 degre

355 MPa

thermomekanikman woule

EN 10028-5

Apatman

 

 

 
P355m pvq asye plak tèmik

 

Tanperati (degre) 32 454 368
Modil Elastisite (GPA) - 139 -
Vle di koyefisyan nan tèmik expaion × 10-6/(degre) - - 23
Tèmik konduktivite (w/m · degre) - 13.3 12.2
Kapasite tèmik espesifik (J/kg · degre) - 241 -
Espesifik rezistivite elektrik (ω mm²/m) 0.44 - -
Divinite (kg/dm³) - - 111
Koyefisyan Poisson a, ν - - 334

 

 
Veso presyon (PVQ) asye plak pwodwi imaj
boiler of steel plate
Boiler Quality Steel Plates
Pressure Vessel Steel
 
Gnee Group Ekip foto

 

China pressure vessel steel manufacturer

 

 
Gnee Gwoup Kliyan Vizit
Boiler Plate Steel
boiler quality steel
pressure vessel plate
Hot rolled boiler steel plates
Boiler grade plates
Boiler plates
 
Gnee Group Steel Egzibisyon
High Temperature Pressure Vessels
vessel steel plate
boiler steel
Pressure Vessel Alloy Plates
China pressure vessel quality steel Distributors
Alloy Steel For Pressure Vessel

Nou gen anplwaye sèvis pwofesyonèl sou entènèt. Si ou gen nenpòt kesyon sou p355m chofaj veso veso asye, tanpri voye nou yon ankèt epi nou pral reponn ou nan yon sèl jou k ap travay.

 

Baj popilè: p355m chofaj presyon veso asye, Lachin p355m chofaj veso veso manifaktirè, founisè, faktori