EN10028-3 P460NH Presyon Steel Plak se asye pou rezon presyon (P) ak fòs sede minimòm de 460 MPa (460) ki te espesifye pwopriyete tanperati ki wo (NH).
Kondisyon pou Tensile
| Epesè pwodwi | Sede fòs MPA | Fòs rupture MPA | Elongasyon A% |
|---|---|---|---|
| jiska 16mm | 460 min | 570 – 730 | 17 min |
| 16mm a 40mm | 445 min | 570 – 720 | 17 min |
| plis pase 40mm a 60mm | 430 min | 570 a 720 | 17 min |
| plis pase 60mm a 100mm | 400 min | 540 a 710 | 17 min |
Pwopriyete mekanik asye P460NH (1.8935)
| Epesè nominal (mm): | rive 16 | 16 - 60 | 60 - 100 |
| Rm - Fòs rupture (MPa) (+N) | 560-730 | 570-720 | 540-710 |
| Epesè nominal (mm): | rive 16 | 16 - 40 | 40 - 60 | 60 - 100 |
| ReH - Minimòm fòs sede (MPa) (+N) | 460 | 445 | 430 | 400 |
| KV - Enèji enpak (J) lonjitid., (+N) | -20 degre 40-45 |
0 degre 47-65 |
+20 degre 55-75 |
| KV - Enèji enpak (J) transverse, (+N) | -20 degre 27-30 |
0 degre 35-40 |
+20 degre 39-50 |


GNEE te sèvi kliyan nan plis pase 50 peyi (Amerik di Nò, Ewòp, Azi Sidès, Mwayen Oryan, elatriye) epi li te genyen eksperyans rich nan tèm komès entènasyonal (FOB, CIF, EXW) ak kondisyon mache lokal yo. Kominikasyon efikas nou an (sipò anglè, panyòl, arab) ak pwosesis biznis transparan fè koperasyon lis epi san pwoblèm-.