ASTM A533 chodyè veso asye disponib nan senk klas fòs diferan: Klas A, Klas B, Klas C, Klas D, ak Klas E. Gen twa nivo nan chak kategori: nivo 1, nivo 2 ak nivo 3.
Dekri teren
Karakteristik teknik

A533 presyon veso chodyè asye plak


Plak veso chodyè ASTM A533 se yon Manganèz-molybdène ak Manganèz-molybdène-nikèl alyaj asye plak apwopriye pou veso presyon soude. Li se anjeneral apwovizyone nan fòm nan trempe ak tanperaman chalè trete (sa vle di, tranzisyon tanperaman). ASTM A533 presyon veso asye disponib nan senk klas fòs diferan: Klas A, Klas B, Klas C, Klas D, ak Klas E. Klas sa yo divize an twa klas: Klas 1, Klas 2, ak Klas 3.

 

Limit epesè siperyè pou klas 1 ak klas 2 ASTM A533 chodyè asye plak limite sèlman pa kapasite konpozisyon chimik la pou satisfè kondisyon espesifik pwopriyete mekanik yo. Sepandan, li se kounye a komen limite epesè nan klas A / B / C / D ASTM A533 plak chodyè a 12 pous, oswa 300 mm, ak epesè a nan klas E ASTM A533 plak chodyè a 7 pous, oswa 180 mm.

 

Pou plak veso klas 3 ASTM A533, epesè maksimòm plak klas A/B/C/D se 2.5 pous, oswa 65 mm, ak epesè maksimòm plak klas E se 2 pous, oswa 50 mm.

 

 
A533 Veso Plak Konpozisyon Chimik

 

eleman   Kategori A Kategori B Kategori C Kategori D Kategori E
C   0.25 0.25 0.25 0.25 0.20
Mn Analiz k ap fonn 1.15~1.50 1.15~1.50 1.15~1.50 1.15~1.50 1.15~1.70
Analiz pwodwi fini 1.07~1.62 1.07~1.62 1.07~1.62 1.07~1.62 1.04~1.84
P   0.025 0.025 0.025 0.025 0.020
S   0.025 0.025 0.025 0.025 0.015
Si Analiz k ap fonn 0.15~0.40 0.15~0.40 0.15~0.40 0.15~0.40 0.15~0.40
Analiz pwodwi fini 0.13~0.45 0.13~0.45 0.13~0.45 0.13~0.45 0.13~0.45
Mo Analiz k ap fonn 0.45~0.60 0.45~0.60 0.45~0.60 0.45~0.60 0.25~0.60
Analiz pwodwi fini 0.41~0.64 0.41~0.64 0.41~0.64 0.41~0.64 0.21~0.64
Ni Analiz k ap fonn … 0.40~0.70 0.70~1.00 0.20~0.40 0.60~1.00
Analiz pwodwi fini … 0.37~0.73 0.67~1.03 0.17~0.43 0.57~1.03
Kr Analiz k ap fonn … … … … 0.60
Analiz pwodwi fini … … … … 0.64

 

 
A533 Chodyè Plak Pwopriyete mekanik

 

ASTM A533 Nivo 1 nivo 2 Nivo 3
ksi (MPa) ksi (MPa) ksi (MPa)
fòs rupture 80-100[550~690] 90-115[620~795] 100-125[690~860]
Sede 50[345] 70[485] 83[570]
Elongasyon, 2 pous [50 mm], % 18 16 16

 

 
Cho woule chodyè asye plak Pwodwi imaj
China pressure vessel plate Distributors
China steel boiler plate Manufacturers
China Boiler Plate Steel Manufacturers
 
Foto ekip gwoup GNEE

 

China pressure vessel steel manufacturer

 

 
Vizit kliyan gwoup GNEE
China boiler plate Distributors
China vessel plate Suppliers
China pvq plate Distributors
China pressure vessel plate Manufacturers
China pressure vessel plate Distributors
China pressure vessel quality steel Suppliers
 
 
GNEE Group asye egzibisyon
China pressure vessel steel manufacturer
China boiler steel plate Manufacturers
China steel boiler plate Distributors
Container steel plate
Pressure Vessel Quality Carbon Steel Plate
Pressure Vessel Quality (PVQ) Steel

Nou gen ase A533 Presyon Veso Chodyè Steel Plak nan stock, epi nou ka tou Customize li selon bezwen ou yo.

 

Baj popilè: A533 presyon veso chodyè asye plak, Lachin A533 presyon veso chodyè asye plak manifaktirè, Swèd, faktori