ASTM A204 Klas C Chodyè Steel Plak

ASTM A204 Klas C Chodyè Steel Plak

Kalite: Plak asye veso
Estanda: AISI, ASTM, DIN, JIS, GB
Teknik: Woule cho
Fòm: Plak
Dekri teren
Karakteristik teknik

ASTM A204 Klas C Chodyè Steel Plak


 

GNEE ofri plak veso presyon A204GrC se plak asye molybdène alyaj pou veso presyon, A204GrC presyon veso plak asye egzekite A204 / A204M-12 estanda. Materyèl plak veso presyon A204GrC nou ofri a gen ekselan konpozisyon chimik ak pwopriyete mekanik, ki ka itilize nan petwòl, pwodui chimik, veso chofaj ak lòt endistri yo.

 

 
Chodyè ak presyon veseel asye plak Pwopriyete chimik

 

Klas

C max

Mn max

Si

Pmax

S max

A204 Klas C

(A204GRC)

0.23

0.98

0.13-0.45

0.035

0.035

 

 

 
Chodyè Kalite Steel Plak pwopriyete mekanik

 

Klas

Fòs rupture (MPa)

Sede fòs (MPa) min

% elongasyon nan 2 pous (50mm) min

Konsekans Tanperati Tès (degre)

A204 Klas C

(A204GRC)

515-655

295

 

20

-20,40,-60

 

 

 

 
Cho woule chodyè asye plak Pwodwi imaj

 

boiler plate

 

 
Foto ekip gwoup GNEE

 

pressure vessel steel

 

 
Vizit kliyan gwoup GNEE

 

pressure vessel plate

 

 
 
GNEE Group asye egzibisyon

 

vessel plate

 

Nou gen ekselan apre-lavant sèvis. Si ou gen nenpòt kesyon sou ASTM A204 Klas C chodyè asye plak, ou ka kontakte nou epi nou pral reponn ou nan de zè de tan.

 

Baj popilè: astm a204 klas c chodyè asye plak, Lachin astm a204 klas c chodyè asye plak manifaktirè, Swèd, faktori