ASTM A203 Klas A Chodyè Steel


 

GNEE ofri A203GrA chodyè asye plak se presyon veso asye plak, A203GrA presyon veso plak egzekitif estanda teknik: ASTM A-203/A-203M.The A203GrA veso asye plak nou ofri yo ka Customized nan gwosè, koupe, soude, pwensonaj ak lòt sèvis pwosesis dapre kondisyon A203G asye A203G.

 

 
Presyon Veso Steel Shell Plak Pwopriyete chimik

 

Klas C Mn Greater than or equal to Si P S
ASTM A203 Klas A (A203GRA) 0.17 0.78-0.88 0.13-0.45 0.035 0.035

 

 
Presyon Veso (PVQ) Steel Plak pwopriyete mekanik

 

Klas Fòs rupture (MPa) Sede fòs (MPa) % elongasyon nan 2 pous (50mm) min Konsekans Tanperati Tès (degre)
ASTM A203 Klas A (A203GRA) 450 255 19 -20,40,-60

 

 
Presyon veso klas asye plak pwodwi imaj

 

boiler steel plate

 

 
Foto ekip gwoup GNEE

 

steel boiler plate

 

 
Vizit kliyan gwoup GNEE

 

Boiler Plate Steel

 

 
 
GNEE Group asye egzibisyon

 

pressure vessel plate

 

Nou gen ekselan apre-lavant sèvis. Si ou gen nenpòt kesyon sou ASTM A203 klas A chodyè asye, ou ka kontakte nou epi nou pral reponn ou nan de zè de tan.

 

Baj popilè: astm a203 klas yon chodyè asye, Lachin astm a203 klas yon chodyè asye manifaktirè, Swèd, faktori