A387 Klas 5 Klas 2 Chodyè Kalite Steel
A387 Gr.5 Cl.2chodyè asye plakse yon plak kwòm-molybdène ki fèt pou resipyan asye kabòn ki ka soude nan tanperati ki wo. Kontni an molybdène bay materyèl la yon adaptabilite tanperati pi pwononse, pandan y ap chromium la bay pi bon rezistans pou itilize.
A387 Gr.5 Cl.2plak veso presyongen yon fòs rupture ant 515 MPa ak 690 MPa, yon fòs sede nan 310 MPa, ak yon elongasyon nan omwen 18%.
A387 Klas 5 Klas 2 Chodyè Plak Steel konpozisyon chimik
| ASTM A387 GR. 5 Cl.1 Plak | |
|---|---|
| Manganèz (Mn) | 0.30 a 0.60 |
| Kabòn (C) | 0.15 |
| Molybdène (Mo) | 0.45 a 0.65 |
| Fosfò (P) | 0.025 |
| Souf (S) | 0.025 |
| Kwòm (Cr) | 4.00 pou 6.00 |
| Silisyòm (Si) | 0.50 |
| Vanadyòm (V) | - |
A387 Klas 5 Klas 2 veso asye plak pwopriyete mekanik
| KLAS | Rediksyon Zòn |
Long. (50mm) |
Fòs Sede (Mpa) |
Fòs rupture (Mpa) |
|---|---|---|---|---|
| ASTM A387 GR 5 CL 2 plak | 40% min | 18% min | 310 min | 515 - 690 |
A387 Klas 5 Klas 2 Plak veso presyon Lis Stock
| Plak Nominal Size Epesè (pous) |
Pwa (lb/ft2) |
|---|---|
| 3/16 pous | 7.65 |
| 1/4 pous | 10.2 |
| 5/16 pous | 12.8 |
| 3/8 pous | 15.3 |
| 7/16 pous | 17.9 |
| 1/2 pous | 20.4 |
| 9/16 pous | 22.9 |
| 5/8 pous | 25.5 |
| 11/16 pous | 28.1 |
| 3/4 pous | 30.6 |
| 13/16 pous | 33.2 |
| 7/8 pous | 35.7 |
| 1 pous | 40.8 |
| 1 1/8 pous | 45.9 |
| 1 1/4 pous | 51.0 |
| 1 3/8 pous | 56.1 |
| 1 1/2 pous | 61.2 |
| 1 5/8 pous | 66.3 |
| 1 3/4 pous | 71.4 |
| 1 7/8 pous | 76.5 |
| 2 pous | 81.6 |
| 2 1/8 pous | 86.7 |
| 2 1/4 pous | 91.8 |
| 2 1/2 pous | 102 |
| 2 3/4 pous | 112 |
| 3 pous | 122 |
| 3 1/4 pous | 133 |
| 3 1/2 pous | 143 |
| 3 3/4 pous | 153 |
| 4 pous | 163 |
| 4 1/4 pous | 173 |
| 4 1/2 pous | 184 |
| 5 pous | 204 |
| 5 1/2 pous | 224 |
| 6 pous | 245 |
| 6 1/2 pous | 265 |
| 7 pous | 286 |
| 7 1/2 pous | 306 |
| 8 pous | 326 |
| 9 pous | 367 |
| 10 pous | 408 |
Cho woule chodyè asye plak Pwodwi imaj



Foto ekip gwoup GNEE

Vizit kliyan gwoup GNEE






GNEE Group asye egzibisyon






Pwodwi nou yo te sibi enspeksyon kalite strik epi yo ekipe ak sètifika pwofesyonèl. Si ou gen nenpòt kesyon sou A387 Klas 5 Klas 2 Chodyè Kalite Steel, ou akeyi yo tcheke.
Baj popilè: a387 klas 5 klas 2 chodyè bon jan kalite asye, Lachin a387 klas 5 klas 2 chodyè bon jan kalite asye manifaktirè, Swèd, faktori