A204 Gr. B Presyon Veso Alloy Plak

A204 Gr. B Presyon Veso Alloy Plak

SA 204 GR B spesifikasyon kouvri plak alyaj molybdène yo, yo patikilyèman apwopriye pou chodyèr soude ak divès kalite lòt kalite veso presyon.
Dekri teren
Karakteristik teknik

A204 Gr. B Presyon Veso Alloy Plak


 

ASTM A204 Klas B se yon klas bon jan kalite chodyè asye. Astm A204 Klas B chodyè Steel Plak yo fèt ak engredyan prim nan kabòn, molybdène, souf Manganèz, fosfò, ak Silisyòm. Konpozan yo entegre nan plak sa yo ba yo rezistans amelyore korozyon ak diminye medya yo. ASTM A204 plak asye alyaj travay byen nan aplikasyon pou presyon ki wo ak tanperati ki wo.

 

Sa204 Gr. Plak veso B gen ekselan pwopriyete mekanik. Plak sa yo gen yon fòs rupture ant 440 ak 590 MPa ak yon fòs sede ant 220 ak 275 MPa. Yo ka alonje pa omwen 19% nan sistèm nan.

 

A204 Klas B plak asye veso yo souvan itilize nan chodyèr endistriyèl, koule chalè veso presyon, ekòs bato, soumaren, ayewospasyal, ak lòt aplikasyon. Tout pwodwi nou yo ka Customized nan kondisyon espesifik kliyan yo.

 

 
A204 klas b chodyè plak konpozisyon chimik

 

Konpozisyon

Kalite

Epesè (mm)

B

C Mwens pase oswa egal a

Analize chalè

Analize pwodwi

Mwens pase oswa egal a 25

0.18

 

 

>25~50

0.21

 

 

>50~100

0.23

 

 

>100

0.25

Mn Less than or equal to

Analiz chalè

-

0.90

 

Analiz pwodwi

-

0.98

P Mwens pase oswa egal a ,S Mwens pase oswa egal a

Analiz chalè

-

0.035

 

Analiz pwodwi

-

0.035

Si

Analiz chalè

-

0.15~0.40

 

Analiz pwodwi

-

0.13~0.45

Mo

Analiz chalè

-

0.45~0.60

 

Analiz pwodwi

-

0.41~0.64

 

 
a204 klas b asye chodyè plak pwopriyete mekanik

 

Klas

Fòs rupture
bo,[MPa]

YieldStrengthmin,
bo,[MPa]

Elongasyon nan 8in.
[200mm],min,%

Elongasyon nan 2in.
[50mm],min,%

A204GrB

65-85[450-585]

37[255]

19

23

 

 
a204 plak veso presyon Tablo pwa

 

Plak epesè
(mm)
Pwa
(kg/m2)
2.0 15.7
1.6 12.6
2.5 19.6
3.2 25.1
3 23.6
4 31.4
6 47.1
5 39.3
10 78.5
8 62.8
12.5 98.1
20 157
15 118
22.5 177
30 236
25 196
32 251
40 314
35 275
45 353

 

 
chodyè asye plak Pwodwi imaj
 
China Boiler Plate Steel Suppliers
China pressure vessel plate Manufacturers
China boiler plate Distributors
 
Foto ekip gwoup GNEE

 

China pressure vessel steel manufacturer

 

 
Vizit kliyan gwoup GNEE
China pressure vessel plate Manufacturers
China pressure vessel quality steel Suppliers
40
China boiler quality plates Suppliers
China pvq plate Suppliers
China vessel plate Manufacturers
 
GNEE Group asye egzibisyon
China pressure vessel steel plate Manufacturers
China carbon steel pressure vessel Manufacturers
China pressure vessel quality steel Distributors
China pressure vessel plate Suppliers
China pressure vessel steel plate Distributors
China carbon steel pressure vessel Manufacturers

Nou gen pèsonèl pwofesyonèl sèvis sou entènèt. Si w gen nenpòt kesyon sou A204 Gr. B Presyon Veso Alloy Plak, tanpri voye nou yon ankèt epi nou pral reponn ou nan yon jou travay.

 

Baj popilè: a 204 gr. b presyon veso alyaj plak, Lachin a204 gr. b presyon veso alyaj plak manifaktirè, Swèd, faktori