Q690E asye se yon kalite asye ki ba alyaj segondè. Yo rele asye Q690E paske nan valè fòs sede li yo, Q se abrevyasyon nan fòs sede, se sa ki, fòs sede Q690E asye se 690 MPa, E endike ke tanperati enpak la. nan Q690E asye se - 40 degre.
Konpozisyon chimik nan materyèl asye Q690E:
C mwens pase oswa egal a {{0}}.18, Si mwens pase oswa egal a 0.60, Mn Mwens pase oswa egal a 2.0 , P mwens pase oswa egal a {{10}}.030, S mwens pase oswa egal a {{20}}.{{24 }}25, Nb Mwens pase oswa egal a 0.11, V Mwens pase oswa egal a 0.12, Ti Mwens pase oswa egal a 0.20, Cr Mwens pase oswa egal a 1.{{ 17}}, Ni mwens pase oswa egal a 0.80, Cu mwens pase oswa egal a 0.80, N mwens pase oswa egal a 0.015, Mo mwens pase oswa egal a 0.30, B mwens pase oswa egal a 0.004, Al mwens pase oswa egal a 0.015.
Q690E materyèl asye pwopriyete mekanik: fòs sede Pi gran pase oswa egal a 690 MPa, fòs rupture 730-940 MPa, elongasyon nan kraze Pi gwo pase oswa egal a 14%, enpak enèji 31J.
Q690E aplikasyon pou materyèl asye:
Q690E materyèl asye gen gwo fòs, bon plastisit ak severite, bon soudabilite, bon pèfòmans cho ak frèt.Materyèl asye Q690E se sitou itilize fabrike yon varyete gwo-echèl jeni estriktirèl konpozan ak machin konstriksyon.
Q690E materyèl asye segondè fòs, severite bon, yo nan lòd yo asire fòs la, rèd ak fyab nan site la, ka diminye pwa a nan eleman yo satisfè eleman yo jeni ak ekipman gwo-echèl, kondisyon ki lejè.