310 asye pur klas yo se kabòn mwayen ki gen asye pur austenitik. Yo gen yon degre nan rezistans korozyon.
Plak SS 310 gen pi gwo tanperati a sèk administrasyon lè nan 1100 ºC.
GNEE STEEL ISO 9001; 2008 Sètifye manifakti nan ASTM A240 Klas 310 Plak & Koulye a, nou te vin distribitè nan Uns S31000 Fèy & DIN 1.4840 Nerjaveèi asye plak.
Espesifikasyon nan asye pur 310 / 310s fèy papye, plak, anwoulman
Espesifikasyon:ASTM A240 / ASME SA240
Dimansyon:ASTM, ASME, ak API.
Lajè:1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, elatriye
Epesè:4mm-100mm
Longè:2000mm, 2440mm, 3000mm, 5800mm, 6000mm, elatriye
Fini sifas:2b, 2d, Ba, No.1, No.4, No.8, 8K, glas, karo, Relief, felen, sandblast, bwòs, grave, cho woule plak (HR), frèt fèy woule (Cr), saten (te rankontre ak plastik kouvwi), elatriye
Fòm:Anwoulman, papye, woulo, fèy plenn, fèy shim, fèy detache, plak karo, teren, plat, vid (sèk), bag (bride), elatriye.
310 / 310s dra asye pur, plak, anwoulman konpozisyon chimik
|
Egalize |
C |
Mn |
Si |
P |
S |
Cr |
Mwa |
NI |
Fe |
|
SS 310 |
0.015 max |
2.0 Max |
0.15 max |
0.020 Max |
0.015 max |
24.00 – 26.00 |
0.10 max |
19.00 – 21.00 |
54.7 min |
|
SS 310s |
0.08 Max |
2.0 Max |
1.00 Max |
0.045 max |
0.030 Max |
24.00 – 26.00 |
0.75 max |
19.00 – 21.00 |
53.095 min |
Nerjaveèi asye 310 / 310s fèy papye, plak pwopriyete mekanik
|
Densite |
Pwen k ap fonn |
Fòs rupture |
Sede fòs (0.2%konpanse) |
Elongasyon |
|
7.9 g/cm3 |
1402 degre (2555 degre f) |
PSI - 75000, MPA - 515 |
PSI - 30000, MPA - 205 |
40 % |
Nerjaveèi asye 310 / 310s fèy papye, plak, anwoulman ekivalan klas
|
Estanda |
WERKSTOFF NR. |
Ògje |
JIS |
BS |
GOST |
Afnor |
En |
|
SS 310 |
1.4841 |
S31000 |
Sus 310 |
310S24 |
20CH25N20S2 |
– |
X15crni25-20 |
|
SS 310s |
1.4845 |
S31008 |
Sus 310s |
310S16 |
20CH23N18 |
– |
X8crni25-21 |
Steel Gnee se youn nan manifakti a ki mennen, ekspòtatè ak founisè nan kalite siperyè ASTM A240 TP310 plak asye pur ak fèy papye. Nou bay yon pakèt domèn plak SS 310 ak fèy papye nan anwoulman, feuilles, woulo, fèy plenn, fèy shim, fèy detache, plak karo, teren, plat, vid (sèk), bag (bride).
Ranje nou an konprann nan plak SS 310 ak fèy papye. Disponib nan dimansyon diferan & klas, sa yo stainlesssteel karo plak ak fèy papye yo lajman itilize nan endistri diferan tankou pouvwa, jeni.Construction ak anpil plis. Nou ofri tou ranje konpetitif nan plak SS 310 ak fèy papye nan kondisyon kliyan.
Gnee asye pur ASTM A240 Tp310 Fèy Komèsyal Ka:
Fèy 2.4mx 1.2mx 6mm ASTM A240 Tp310, lis materyèl asye pur: ASTM A240 TP310, Dimansyon: 2.4m longè x 1.2m lajè x 6mm epesè
Atik pwodwi: fèy tiyo
Materyèl: ASTM A240 TP310
Dimansyon: 2.4mx 1.2mx 6mm
Materyèl: lis asye pur, ASTM A240 TP310
Gwosè: 2.4 mèt
Lajè: 1.2 mèt
Epesè: 6 mm

Avèk yon sifas ki lis, yon longè 2.4 mèt, yon lajè nan 1.2 mèt, ak yon epesè nan 6mm, fèy papye nou yo se chwa pafè a pou bezwen endistriyèl ou oswa komèsyal yo. Lòd kounye a epi fè eksperyans durability a ak fòs nan segondè nou an - bon jan kalite dra asye pur.
Kap chèche yon founisè serye asye pur? Gade pa gen plis pase ASTM A240 nou an TP310 dra asye pur!
|
Klas asye ekivalan dapre lòt estanda pou ASTM A 240 310 s |
|||||||
|
Non |
JIS G4304 |
Astm |
Ògje |
K |
EN10095 |
Tankou |
CNS |
|
1 |
Sus201 |
201 |
S20100 |
STS201 |
1.4372 |
201-2 |
201 |
|
2 |
Sus202 |
202 |
S20200 |
STS202 |
1.4373 |
- |
202 |
|
3 |
Sus301 |
301 |
S30100 |
STS301 |
1.4319 |
301 |
301 |
|
4 |
Sus304 |
304 |
S30400 |
STS304 |
1.4301 |
304 |
304 |
|
5 |
Sus304l |
304L |
S30403 |
STS304L |
1.4306 |
304L |
304L |
|
6 |
Sus304n1 |
304N |
S30451 |
STS304N1 |
1.4315 |
304N1 |
304N1 |
|
7 |
Sus304n2 |
Xm21 |
S30452 |
STS304N2 |
- |
304N2 |
304N2 |
|
8 |
Sus304ln |
304ln |
S30453 |
STS304LN |
- |
304ln |
304ln |
|
9 |
Sus305 |
305 |
S30500 |
STS305 |
1.4303 |
305 |
305 |
|
10 |
Sus309s |
309S |
S30908 |
STS309S |
1.4833 |
309S |
309S |
|
11 |
Sus310s |
310S |
S31008 |
STS310s |
1.4845 |
310S |
310S |
|
12 |
Sus316 |
316 |
S31600 |
STS316 |
1.4401 |
316 |
316 |
|
13 |
Sus316ti |
316ti |
S31635 |
- |
1.4571 |
316ti |
316ti |
|
14 |
Sus316l |
316L |
S31603 |
STS316L |
1.4404 |
316L |
316L |
|
15 |
Sus316n |
316N |
S31651 |
STS316N |
- |
316N |
316N |
|
16 |
Sus316ln |
316ln |
S31653 |
STS316LN |
1.4429 |
316ln |
316ln |
|
17 |
Sus316j1 |
- |
- |
STS316J1 |
- |
316J1 |
316J1 |
|
18 |
Sus316j1l |
- |
- |
STS316J1L |
- |
- |
316J1L |
|
19 |
Sus317 |
317 |
S31700 |
STS317 |
- |
317 |
317 |
|
20 |
Sus317l |
317L |
S31703 |
STS317L |
1.4438 |
317L |
317L |
|
21 |
Sus321 |
321 |
S32100 |
STS321 |
1.4541 |
321 |
321 |
|
22 |
Sus347 |
347 |
S34700 |
STS347 |
1.455 |
347 |
347 |
|
23 |
Sus329j1 |
329 |
S32900 |
STS329J1 |
1.4477 |
329J1 |
329J1 |
|
24 |
Sus329j3l |
- |
S31803 |
STS329J3L |
1.4462 |
329J3L |
329J3L |
|
25 |
Sus405 |
405 |
S40500 |
STS405 |
1.4002 |
405 |
405 |
|
26 |
Suh409 |
409 |
S40900 |
STS409 |
1.4512 |
409L |
409L |
|
27 |
Sus410l |
- |
- |
STS410L |
- |
410L |
410L |
|
28 |
SUS430 |
430 |
S43000 |
STS430 |
1.4016 |
430 |
430 |
|
29 |
Sus434 |
434 |
S43400 |
STS434 |
1.4113 |
434 |
434 |
|
30 |
- |
- |
S43940 |
- |
1.4509 |
439 |
439 |
|
31 |
Sus444 |
444 |
S44400 |
STS444 |
1.4521 |
444 |
444 |
|
32 |
Sus403 |
403 |
S40300 |
STS403 |
- |
403 |
403 |
|
33 |
Sus410 |
410 |
S41000 |
STS410 |
1.4006 |
410 |
410 |
|
34 |
Sus420j1 |
420 |
S42000 |
STS420J1 |
1.4021 |
420 |
420J1 |
|
35 |
Sus420j2 |
- |
- |
STS420J2 |
1.4028 |
420J2 |
420J2 |
|
36 |
Sus440a |
440A |
S44002 |
STS440A |
- |
440A |
440A |