Atik pwodwi: fòje disk asye, disk koupe soti nan ba fòje
Materyèl: ASME SB564 UNS N06625/Inconel 625
Dyamèt: 200 mm
Epesè: 30 mm
NACE Kondisyon: NACE MR0103
Dite:<35 HRC
Se inconel 625 disk la fòje te fè soti nan segondè - bon jan kalite ASME SB564 UNS N06625 Materya. Avèk yon dyamèt 200 mm ak yon epesè nan 30 mm, disk sa a se presizyon koupe soti nan yon bar fòje asire durability ak disponiblite.
Li satisfè kondisyon yo NACE sevè MR0103, fè li ideyal pou itilize nan sèvis gaz tounen ak lòt aplikasyon pou difisil.
Inconel materyèl ekivalan ak deziyasyon
| Inconel 600 | EN/DIN 2.4816 | UNS N06600 | Alyaj 600 |
| Inconel 625 | EN/DIN 2.4856 | UNS N06625 | Alloy 625 |
| Inconel 718 | EN/DIN 2.4668 | UNS N07718 | Alloy 718 |
Inconel 625 Forging pwodwi ki gen rapò ak asye goudwon
| Alloy 625 fòje bag | Inconel Alloy 625 fòje bag |
| Inconel 625 fòje disk | Inconel Alloy 625 fòje disk |
| Inconel 625 fòje bag | Alyaj 625 rasin |
| Inconel alyaj 625 Forgings | Inconel 625 rasin |
| Alloy 625 fòje ba | ASTM B446 alyaj 625 rasin |
| ASTM B446 alyaj 625 bag fòje | ASTM B446 Alloy 625 Forgings |
| Inconel Alloy 625 fòje ba | Alyaj 625 bag |
| ASTM B446 Alloy 625 bag | Inconel alyaj 625 rasin |
| ASTM B446 alyaj 625 disk fòje | ASTM B446 Alloy 625 Fòje ba |
| Alloy 625 Forgings | Inconel 625 Forgings |
| Inconel 625 fòje ba | Inconel 625 bag |
| Inconel alyaj 625 bag |
Inconel 625 fòje disk ASME SB564 UNS N06625 FORGED bag
Nou se manifakti pwofesyonèl nan Inconel 625 fòje disk ASME SB564 UNS N06625 fòje bag nan peyi Lachin.
Ki sa ki se yon disk fòje?
Yon disk fòje se tipikmanyon sèl - pyès eleman solid, fòm wonn, jis tankou yon disk, kote OD a depase gwosè a longè.
Se pwosesis la tou, yo itilize yo kreye disk asye gwo pou itilize nan ekipman endistriyèl, tiyo ak lòt segondè - konpozan presyon pou lwil yo, gaz ak endistri petrochimik.
Inconel 625 disk
Inconel 625 se yon nikèl - ki baze sou superalloy li te ye pou fòs segondè li yo ak rezistans nan presyon, oksidasyon, ak korozyon.
Inconel 625 èl, alyaj 625, UNS N06625 klas ekivalan
| Estanda | WERKSTOFF NR. | Ògje | JIS | BS | GOST | Afnor | En | Ou |
| Inconel 625 | 2.4856 | N06625 | NCF 625 | NA 21 | ХН75МБТЮ | Nc22dnb4m | NICR22MO9NB | ЭИ602 |
Inconel 625 konpozisyon chimik
| Egalize | C | Mn | Si | P | S | NI | Cr | Fe | Mwa | CO | Al | Ti | Nb + ta |
| Inconel 625 | 0.10 max | 0.50 max | 0.50 max | 0.015 max | 0.015 max | 58.0 min | 20.0 – 23.0 | 5.0 Max | 8.0 – 10.0 | 1.0 Max | 0.40 max | 0.40 max | 3.15 – 4.15 |
Alyaj 625 pwopriyete mekanik
| Densite | Pwen k ap fonn | Fòs rupture | Sede fòs (0.2%konpanse) | Elongasyon |
| 7.94 g/cm3 | 1385 degre (2525 degre F) | PSI - 75,000, MPA - 520 | PSI - 30,000, MPA –205 | 30 % |
Nou se pwofesyonèl fòje disk, fòje disk, fòje disk, tou, tankou disk, asye fòje disk, asye fòje disk, asye fòje/fòje disk faktori ki soti nan Lachin
Metòd la k ap fonn nan fòje materyèl se ESR+Vir oswa Vim+ESR+var
Kòm pou chak fòje nan materyèl, nou gen 1 tòn, 3 tòn, 6 tòn, 9 tòn louvri mouri tou, ak 4500 tòn laprès idwolik.
Nou ta ka fè rkwit tretman, normalized, redi ak tanperaman tretman pou fòje ki gen kapasite, fòje ki gen kapasite tankou pou kondisyon an nan kliyan yo.
Folllowing se klas la asye nan tou, tankou disk, fòje ki gen kapasite ke nou ta ka fè:
Alloy ak kabòn asye fòje nòt asye:
A182-F1, A182-F2, A182-F9, A182-F11, A182-F12, A182-F21, A182-F22, A182-F36, A182-F91, A182-F92, A694-F42, A694-F46, A694-F48, A694-F50, A694-F60, A694-F70, SA-350 LF1, SA-350 LF2, SA-350 LF3, SA-350 LF5, SA-350 LF6, AISI 1045, AISI 4140, AISI 4130, AISI 4340, AISI 4317, AISI 4130, AIS 4340, AIS 4317, AISI 4130, AIS 4340, AISI 4317, AISI 4130, AIS 4340, AISI 4317, AISI 4130, AIS 4340, AISI 4317, AIS 4130, 4145H, AISI 4145H, AISI 4145H MOD, AISI 4330V, AISI 4330V MOD. AISI 4150, AISI 1020, 42CRMO4, 25CRMO4, 34CRNIMO6, 17CRNIMO 6-4 20 NICRMO22, 34CRMO4, 30CRNIMO8, 36CRNIMO4, 12crmo9-10, 18crmos4, 18crnimo7-6, 17crnimo6, 16mncr5, st52-3, s355j2g3, 50crmo4, 39nicrmo3 ,, 20NICRMO2-2
Nerjaveèi asye fòje klas asye
A182-F6A, A182-F6B, A182-F304, A182-F304L, A182-F310, A182-F316, A182-F316L, A182-F317, A182-F317L, A182-F347, AISI 309, AIS-F317L, A182-F347, AISI 309, AIS-F317L, A182-F347, AISI 309, AIS-F317L, A182-F347, AISI 309, AIS-F317L, A182-F347, AISI 309, AIS-F317L, A182-F347, A182-F48, A182-F321, A182-F347, A182-F348, Nitronic 50, Nitronic 40, Nitronic 60, Nitronic 30, Xm-11, Xm-10, UNS S21800, Alloy 20, 904L, PH13-8Mo, 17-4ph, 15-5ph, 17-7ph, Ph15-7 Mo, 254SMO, AL-6XN, 654SMO, A182-F44, A182-F45, A182-F51, A182-F53, A182-F60, A182-F55, A182-F62, A182-F522-F52
Alyaj nikèl ak alyaj super fòbe asye klas
Nickel 200, Nickel 201, Monel 400, Monel R-405, Monel K-500, Hastelloy C-22, Hastelloy X, Hastelloy C-4, Hastelloy B-2, Hastelloy C-276, Hastelloy C-2000, Hastelloy B, Nimonic 75, Nimonic 90, Nimonic 80A, Nimonic 105, Nimonic 901, Inconel 600, inconel 601, inconel 617, inconel 625, inconel 686, inconel 690, inconel 693, inconel 718, inconel 725, inconel X-750, incoloy 800, incoloy 800H, incoloy 800HT, Incoloy 825, Incoloy 926, Incoloy 890, Incoloy 925, Incoloy 901, Incoloy 945, Incoloy A-286, NI-SPAN-C Alloy 902, MP35N, MP159, Multimet N155, Haynes 230, Haynes 188, Haynes 25, Udimet 500, Rene 41, Waspalloy, Invar 36, Invar 42, Stellite 6B, Kovar alyaj,
UNS NO6022, UNS NO6200, UNS No5500, UNS NO6002, UNS N010665, UNS N10276, UNS N10001, UNS N07080, UNS N06600, UNS N06601, UNS NO6625, UNS N06686, UNS N06693, UNS N06690, UNS N07718, UNS N07725, UNS N07750, UNS N08800, UNS N08811, UNS N08810, UNS N08825, UNS N09925, UNS S66286, UNS N07500, UNS K93600
2.4602, 2.4675, 2.4816, 2.4663, 2.4642, 2.4668, 2.4669, 1.4958, 2.4858, 2.4375, 2.4665, 2.4617, 2.4819. 2.4631, 2.4851, 2.4606, 1.4876, 1.4959, 1.4980, 2.4983, 2.4656
Zouti ak mouri asye fòje nòt asye
AISI 6F7, AISI A2, AISI O1, AISI O2, AISI S7, AISI D6, AISI S1, AISI D2, AISI A6, AISI O7, AISI L2, H13, H11, H12, P 20+ ni, p 20+ s, s136, 718
SKT6, SKD12, SKD1, SKD2, SKS3, SKS41, SKS95, SKD11, DC53, SKS43, SKD61, SKD6, SKT4, SKD5, SKD7, SKD62, NAK80
1.2767, 1.2363, 1.2510, 1.2080, 1.2436, 1.2542, 1.2379, 1.2824, 1.2550, 1.2509, 1.2210, 1.2344, 1.2606, 1.2782, 1.2678, 1.2889, 1.2605, 1.2343, 1.2714, 1.2581, 1.2365, 1.2779, 1.2661, 1.2083, 1.2311, 1.2312, 1.2738, 1.2316
Tretman chalè:
Normalize / rkwit / pasè / apeze
Tretman sifas:
Penti, PLATING, polisaj, oksid nwa, transparan anti - lwil oliv rouye
Kontwòl Kalite:
UT, MT, RT, PT, tès konpozisyon chimik, tès pwopriyete mekanik, elatriye.
Enspeksyon:
1, sètifika materyèl anvan tout koreksyon (konpozisyon chimik materyèl) 2, Rapò fèy tretman chalè
3, Rapò enspeksyon dimansyon 4, rapò tès UT
Kondisyon livrezon:
Cho fòje + ki graj machinèd (sifas nwa apre Q /t) + vire