Pwodwi Atik: Asye Plak, S690Q Steel Plak, Q960E Steel Plak, Q690E Steel Plak, Low Alloy High Force Steel Plak
Segondè fòs asye: Q690D, Q690E, Q960E, S690Q, S690QL, S960Q, S960QL, S960QL1
Lajè: 2500mm
Longè: 12000mm
Epesè: 40mm
Dimansyon: ta ka selon gwosè kliyan an

Gamme nou an gen ladan klas Q690D, Q690E, Q960E, S690Q, S690QL, S960Q, S960QL, S960QL1.
Dimansyon Custom disponib tou. Ogmante pwojè ou yo ak plak asye ki gen bon jan kalite-wo-fòs.
Segondè plak asye fòs S690QL, Q690E, STRENX 700 E ak Weldox 700E se tout klas asye ekivalan ki mande enpak tanperati tès nan - 40 degre santigrad ak valè minimòm de enpak enèji nan 30 J sou moso tès longitudinal V-dan. S690QL, asye plak STRENX 700 E ak asye plak Weldox 700E.
Steel plak Q690E soti nan spesifikasyon asye Chinwa GB/T 16270-2009 Plak asye estriktirèl segondè fòs nan kondisyon an trempe ak tanperaman.
Dapre diferan fòs rupture ak tanperati tès enpak, gen kalite asye Q460C asye plak, Q460D asye plak, Q460E asye plak, Q460F asye plak, Q500C asye plak, Q500D asye plak, Q500E asye plak, Q500F asye plak, Q550C asye plak, Q550C asye plak, asye Q550D50F plak, Q620C asye plak, Q620D asye plak, Q620E asye plak, Q620F asye plak, Q690C asye plak, Q690D asye plak, Q690E asye plak, Q690F asye plak, Q800C asye plak, Q800D asye plak, Q800E asye plak, Q800F asye plak, Q800F asye plak, asye Q800F plak, plak asye Q890E, plak asye Q890F, plak asye Q960C, plak asye Q960D, plak asye Q960E, plak asye Q960F.
Se plak asye S690QL pwodwi konfòme yo ak EN estanda EN 10025-6 spesifikasyon, Hot woule segondè fòs sede estriktirèl asye nan kondisyon an trempe ak tanperaman. plak asye, plak asye s550QL, plak asye S550QL1, plak asye S620Q, plak asye s620QL, plak asye S620QL1, plak asye S690Q, plak asye s690QL, plak asye S690QL1, plak asye S890Q, plak asye s890QL, plak asye s890QL, asye plak S890L96L plak.


STRENX 700 E ak Weldox 700E se pi wo plak asye fòs rupture ki te pwodwi pa SSAB, epesè plak ranje soti nan 4 - 160mm (0.157 '' a 6.299 '') aplikasyon tyoical gen ladan egzijan estrikti portant chaj. fèy, STRENX 700MC F plak asye, STRENX 700MC PLUS fèy asye, STRENX 700 OME plak asye, STRENX P700 plak asye, STRENX 700 CR fèy asye, bobin ak bobin fann.
Deskripsyon Product
|
Non pwodwi |
10mm 8mm Q690d Q690e Q960e Q960d plak asye mekanik Jeni Weldox900 Astm A572gr50 A573gr70 gwo fòs plak asye |
|
Lajè |
0.6m-3m oswa jan sa nesesè |
|
Longè |
4m-12m oswa jan sa nesesè |
|
Epesè |
3mm-300mm oswa jan sa nesesè |
|
Estanda |
AISI, ASTM, DIN JIS, GB, SUS, EN, elatriye. |
|
Tretman andigman |
Dapre kondisyon kliyan |
|
Materyèl |
BS600MC BS650MC BS700MC BS750MC S690QL S890 S1080 WELDON700/900 S460M/ML S460Q/QL S500Q/QL S550Q/QL S620Q/QL S690Q/QL S890Q/QL Q460C/D/E Q500C/D Q500E Q550C/D Q620C/D/E Q800C/D Q890C/D |
|
GB |
Q355 A/B/C/D/E, Q420 A/B/C/D/E, Q460 D/E, Q550QD |
|
DIN 17100 |
St37 |
|
ASTM |
A709Gr.36/50/50W, A678GrA/B/C, A572Gr.50/55/60/65, A573Gr.58/65/70, A633Gr. A/C/D |
|
EN10025 |
S355JR, S355NL, S355ML, S355M, S355JR/JO/J2/K2 |
|
JIS |
SS490 A/B/C, SS520 B/C, SM570, SS490, SS540 |
|
Aplikasyon |
Sitou itilize nan ekipman, konstriksyon, otomobil, endistri pétrochimique, gwo bato, pon, ekipman estasyon elektrik, chodyè presyon mwayen ak segondè, veso presyon wo, materyèl woule, machin leve, machin min ak lòt gwo pati estriktirèl soude. |
|
MOQ |
25tons.We tou ka aksepte echantiyon lòd. |
|
Steel/Klas |
Estanda |
Gwosè Range |
Kondisyon livrezon |
|
Q420B/C/D/E |
GB/T1591 |
Mwens pase oswa egal a 150 |
TMCP/N |
|
S460M/ML |
EN10025-4 |
Mwens pase oswa egal a 100 |
TMCP |
|
S460Q/QL/QL1 |
EN10025-6 |
Mwens pase oswa egal a 150 |
Q+T |
|
S460N/NL |
EN10025-3 |
Mwens pase oswa egal a 200 |
N |
|
Q500C/D/E |
G8/T 1591 |
150 |
TMCP/Q+T |
|
Q550C/D/E |
GB/T 1591 |
Mwens pase oswa egal a 150 |
TMCP/Q*T |
|
Q690C/D/E |
GB/T16270 |
Mwens pase oswa egal a 220 |
Q+T |
|
S690Q/QL/QL1 |
EN 10025-6 |
Mwens pase oswa egal a 220 |
Q+T |
|
QB90C/D/E |
GB/T16270 |
Mwens pase oswa egal a 150 |
Q+T |
|
Q890Q/QL/QL1 |
EN 10025-6 |
Mwens pase oswa egal a 150 |
Q+T |
|
Q960C/D/E |
GB/T 16270 |
Mwens pase oswa egal a 100 |
Q+T |
|
S960Q/QL |
EN 10025-6 |
Mwens pase oswa egal a 100 |
Q+T |
|
A514GrB/E/F/H/Q |
ASTM A514 |
Mwens pase oswa egal a 200 |
Q+T |
Q690d Q690e Q960e Q960d Steel Plak Mechanical Engineering Weldox900 Astm A572gr50 A573gr70 High Force Steel Plak Gen gwo Sede ak fòs Tensile epi li lajman ki itilize nan machin min chabon
Pwopriyete prensipal yo nan plak asye segondè fòs yo se gwo fòs, espesyalman nan nòmalizasyon oswa nòmalizasyon ak tanperaman eta a, ki gen pi wo pwopriyete mekanik konplè.
Plak asye ki gen gwo -fòs gen pi wo estrès sede ak fòs rupture, ak fòs yo jeneralman pi wo pase sa yo ki nan plak asye òdinè, anjeneral, ant 350-1000MPa, pandan y ap fòs nan plak asye òdinè se jeneralman ant 200-350MPa.
Fòs segondè sa a se akòz mikwostrikti ki pi dans nan plak asye ki gen gwo -fòs ak grenn ki pi rafine, ki amelyore pwopriyete yo mekanik an jeneral nan materyèl la. An tèm de konpozisyon, anplis fè, kabòn, Manganèz ak lòt eleman, gwo -plak asye fòs tou ajoute lòt eleman alyaj tankou Silisyòm, fosfò, nikèl, elatriye amelyore pwopriyete mekanik yo ak rezistans korozyon.
Plak asye segondè fòs S690Q Q690D Q690E Q960E S690Q Pwodwi detaye