Dènyèman, GNEE STEEL te resevwa yon lòd ijan nan men yon antrepriz chimik Vyetnamyen, ki egzije rezèv pou 150 tònQ345R presyon veso asye plaknan 10 jou pou antretyen an ijans nan plant asid acetic li yo. Konpayi an imedyatman aktive plan pwodiksyon ijans la epi finalman fini livrezon an 1 jou anvan orè a.

Akòz yon echèk toudenkou nan plant la, kliyan Vyetnamyen an ijan te bezwen ranplase koki veso presyon domaje a epi kontakte GNEE atravè Chanm Komès Lachin nan Vyetnam. "Si machandiz yo pa rive nan 10 jou, tout liy pwodiksyon an pral fèmen, sa ki lakòz yon pèt chak jou nan plis pase yon milyon Yuan!" direktè akizisyon kliyan an te di ak kè sote nan telefòn lan. GNEE imedyatman kowòdone: atelye matyè premyè a te bay priyorite pou asiyen billets asye espesyal pou Q345R (konfòme ak estanda GB/T 3531, ak yon fòs sede ki pi gran pase oswa egal a 345MPa, yon fòs rupture nan 470-630MPa, delivre nan kondisyon nòmal, tanperati enpak nan 0 degre pi gwo pase 3, oswa enpak enèji egal a 4, oswa egal a J); atelye a woule asye ajiste plan pwodiksyon an; ak depatman an enspeksyon kalite ansanm te pote soti "enspeksyon pandan pwodiksyon an".
Pandan peryòd pwodiksyon an, kliyan an te fè aranjman pou yon moun devwe pou yo estasyone nan faktori GNEE pou swiv pwogrè a an tan reyèl. Lè yo te wè ke plak asye yo te pwodwi nan 8yèm jou a ak tout tès twazyèm -pati (ki gen ladan tès rupture, koube, ak enpak) te pase, reprezantan kliyan an te fè yon soupi: "Efikas pwodiksyon an ak sans responsablite nan moulen asye Chinwa yo te depase atant!" Pakèt sa a nan plak asye Q345R (spesifikasyon: 14-22mm × 2000-2800mm × 6000-9000mm) ranpli rapid clearance koutim nan pò a Pingxiang nan Guangxi e li te san pèdi tan delivre nan faktori a Vyetnamyen, asire reouvè nan pwodiksyon an nan plant la.
Livrezon ijans sa a pa sèlman redwi pèt fèmen kliyan an, men tou li te ede plak asye GNEE Q345R etabli yon imaj "founisè serye" nan mache chimik Sidès Azyatik la.
Klike pou jwenn yon echantiyon gratis
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.
Ki sa ki ekivalan Q345R?
Q345R se yon lajman itilize asye alyaj ba yo bati veso presyon nan Lachin, egal aASTM A516/A516M klas 70 mwayen kabòn asye. Plak Q345R yo rele plak asye presyon veso pafwa.
Ki sa ki materyèl Q345R?
Q345R sekomen asye alyaj ba, li se chodyè pwesyon zanj lan vide gode ki souvan itilize en kalite, eta livrezon: cho woule oubyen nòmalizasyon.
Ki diferans ki genyen ant Q345R ak Q345B?
1. Q345B materyèl: Li se yon asye alyaj ki ba kabòn (c<0.2%), with good comprehensive performance, good low temperature performance, cold stamping performance, welding performance and machinability.
2. Q345R materyèl: Li se yon plak espesyal pou veso presyon ak yon fòs sede nan 345MPa.
Ki sa ki spesifikasyon asye Q345?
Q345 a se yon asye akmwens pase 0.2 pousan nan konpozisyon li yo fèt ak kabòn, mwens pase 0.55 pousan nan konpozisyon li yo te fè nan Silisyòm ak plizyè enpurte. Sa a klas patikilye nan asye se yon objektif jeneral fabrikasyon asye nan jaden ekipman konstriksyon.
Ki diferans ki genyen ant Q345R ak Q245R?
Diferans ant Q345R ak Q245R Steel Plak
Pou egzanp: Li evidanQ345R gen avantaj sou fòs sede veso presyon; pandan y ap Q245R montre avantaj sou Kalkil rèd veso, ak pou Q245R se asye kabòn, li gen avantaj pri konpare ak asye alyaj ki ba -Q345R.
| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Klas3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||