Plak asye P355NL1 se yon plak asye pou veso presyon estanda Ewopeyen an. Li pwodui dapre estanda Ewopeyen an EN10028. Se plak asye a fèt pa fusion konvètisè oswa raffinage founo elektrik. Li se yon asye ki touye amann. Q355NL1 gen rezistans fatig, rezistans tanperati ki ba ak gwo sede. Fòs ak severite. P355NL1 plak asye klas endikasyon: "P": endike plak veso estanda Ewopeyen an; "355": endike ke fòs sede minimòm plak asye a se 355, nan MPa; "NL1": endike ke plak asye a se yon espesyal kalite asye ba-tanperati.
Konpozisyon chimik % asye P355NL1 (1.0566):
| C | sizo | Mn | Ni | P | S | Kr | Mo | V | N | Nòb | Tibèkil | al | Taks | - |
| max 0.18 | max 0.5 | 1.1 - 1.7 | max 0.5 | max 0.025 | max 0.015 | max 0.3 | max 0.08 | max 0.1 | max 0.012 | max 0.05 | max 0.03 | max 0.02 | max 0.3 | Nb+Ti+V < 0.12 |
Pwopriyete mekanik asye P355NL1 (1.0566):
| Epesè nominal (mm): | rive 60 | 60 - 100 | 100 - 150 | 150 - 250 |
| Rm- Fòs rupture (MPa) (+N) | 490-630 | 470-610 | 460-600 | 450-590 |
| Epesè nominal (mm): | rive 16 | 16 - 40 | 40 - 60 | 60 - 100 | 100 - 150 | 150 - 250 |
| repete- Minimòm fòs sede (MPa) (+N) | 355 | 345 | 335 | 315 | 305 | 295 |
| KV- Enèji enpak (J) transverse, (+N) | -40 degre 27 |
-20 degre 35 |
0 degre 43-50 |
+20 degre 47-60 |
| KV- Enèji enpak (J) lonjitid., (+N) | -50 degre 30 |
-40 degre 40 |
-20 degre 50-53 |
0 degre 65-70 |
+20 degre 70-80 |
| Epesè nominal (mm): | rive 60 | 60 - 250 |
| A- Min. elongasyon nan ka zo kase (%) (+N) | 22 | 21 |