DH-36 plak asye naval ak pwofil anpoul pou yon pwojè naval nan Kolonbi
| Sijè | Deskripsyon | Epesè mm |
| 1 | Naval Steel Fèy DH 36 - 6, 34 mm x 2438,4 mm x 12192 mm (8 pye x 20 pye) | 6.34 |
| 2 | Naval Steel Fèy DH 36 - 25 mm x 2438,4 mm x 12192 mm (8 pye x 20 pye) | 25 |
| 3 | Naval Steel Fèy DH 36 - 50 mm x 2438,4 mm x 12192 mm (8 pye x 20 pye) | 50 |
| 4 | Bulb Profile Gra (ABS) 220 mm x 10 mm x 12 mèt | 10 |
| 5 | Kare pwofil asye a 36 - 6, 35 mm thk x 31,7 mm x 31,7 mm x 12 mèt | 6.35 |