Atik pwodwi: fèy tib, alyaj kwiv tubesheet, chalè echanjeur kwiv alyaj tubesheet
Materyèl: Copper alyaj UNS C70600, Nikèl Copper (90:10), Copper Alloy Uns C70600, Cuni10fe1mn, CW352H, Nikèl Copper (90:10), BS 2871
Dimansyon: Dapre desen kliyan an
Gnee - Yon founisè fèy ki mennen nan kwiv alyaj nan peyi Lachin.
Fèy tib UNS C70600 nou an, manifaktire soti nan Copper Alloy Cuni10fe1mn (CW352H) tankou pou chak BS 2871 estanda, se pwepare a dimansyon egzak jan sa espesifye nan kliyan an.
Ki fèt espesyalman pou aplikasyon pou dlo lanmè, li ofri eksepsyonèl rezistans korozyon ak rezistans. Ideyal pou anviwònman maren, fèy la tib asire pèfòmans serye ak lonjevite, satisfè estanda bon jan kalite sevè sipòte pwosesis kritik endistriyèl ki mande rezistans gaya nan korozyon dlo lanmè.
Nou ofri dimansyon Customized dapre desen kliyan yo, ki espesyalize nan UNS C70600, Cuni30Fe1MN, ak BS 2871 alyaj, li te ye pou lanmè eksepsyonèl yo - rezistans korozyon dlo.
UNS C70600 klas ekivalan
| GB | ISO | Astm | JIS |
| BFE10-1-1 | Cuni10fe1mn | C70600 | C7060 |
C70600 Nikèl Copper (90/10)
Ekivalan: DIN 17664, 2.0882, Cuni10fe1mn
ASTM B171 UNS C70600 CUNI 90/10 COPPER ALLOY TUBESHEET POU echanje
TubeSheet a se eleman nan sipò nan echanjeur la chalè ak chofaj. Fèy papye tib yo vini nan diferan gwosè epi yo trou ak yon seri de twou yo kreye yon kote pou soude fini yo tib. Gen de kalite komen nan tubesheet: fèy papye k ap flote ak fèy estasyonè tib.
UNS C70600 Copper Alloy Espesifikasyon
| Fen pwodwi | Spesifikasyon |
|---|---|
| Baro | ASTM B151, B122, Militè Mil - C-15726 |
| Tiyo, san pwoblèm | ASME SB466, ASTM B466 |
| Tiyo, soude | ASME SB467, ASTM B608, B467 |
| Asyèt | ASTM B122, militè mil - C-15726 |
| Plak, rekouvèr | ASTM B432 |
| Plak, tib kondansateur | ASME SB171, ASTM B171, SAE J463, J461 |
| Baton | ASTM B151, militè mil - C-15726 |
| Baton, soude | AWS A5.15 |
| Dra | ASTM B122, Militè Mil - C-15726, SAE J463, J461 |
| Teren | ASTM B122, militè mil - C-15726 |
| Tib, kondansateur | ASME SB111, ASTM B552, B111, Militè MIL - T-15005, SAE J463, J461 |
Klas materyèl nan tubeSheet
| Kalite materyèl | Kondisyon teknik dapre |
| Duplex asye pur | ASTM/ASME SA182 F44, F45, F51, F53, F55, F60, F61 |
| Asye pur | ASTM/ASME SA182 F304,304L, F316,316L, F310, F317L, F321, F347 |
| Asye kabòn | ASTM/ASME A105, A350 LF1, LF2, A266, A694, A765 Gr.2 |
| Asye alyaj | ASTM/ASME SA182 F1, F5, F9, F11, F12, F22, F51, A350-LF3 |
| Titaniom | ASTM/ASME SB381, Gr.1, Gr.2, Gr.5, Gr.7, Gr.12, Gr.16 |
| Nikèl kwiv | ASTM/ASME SB151, UNS 70600 (Cu - Ni 90/10), 71500 (Cu - Ni 70/30) |
| Kwiv, al - kwiv | ASTM/ASME SB152 UNS C10100, C10200, C10300, C10800, C12200 |
| Alyaj nikèl | ASTM/ASME SB169, SB171, SB564, UNS 2200, UNS 4400, UNS 8825 UNS 6600, UNS 6601, UNS 6625 |
| Alyaj 20 | ASTM/ASME SB472 UNS 8020 |
| Hastelloy | ASTM/ASME SB564, UNS10276 (C 276) |
| Materyèl Claded | ASTM/ASME SB898, SB263, SB264 oswa pi pre CLADDING eksplozyon, fè materyèl nan 2 nan 1 oswa 3 nan 1. |
| Titanium - Steel, Nikèl - Steel, Titàn - Copper, Nerjaveèi asye - asye kabòn, alyaj - asye elatriye. |
Gen kèk aplikasyon komen nan tubeSheets:
1. echanjeur chalè
2. Chodyè
3. kondansateur
4. Reyaktè
5. Lwil ak endistri gaz
6. èkondisyone ak refrijerasyon
7. Veso presyon