ASTM A285 PVQ Steel Plak

Apr 11, 2024 Kite yon mesaj

Estanda ASTM A285 la aplike pou asye kabòn, plak asye ki ba ak mwayen rupture pou veso presyon fizyon -soude.


Plak asye anba ASTM A285 yo klase nan twa klas, A, B, ak C, ak ASTM A285 Klas C ki pi souvan itilize.

 

Konpozisyon chimik ASTM A285:

ASTM A285 konpozisyon chimik Klas A Klas B Klas C
Kabòn, max 0.17 0.22 0.28
Manganèz, max 0.90 0.90 0.90
Fosfò, max 0.035 0.035 0.035
Souf, max 0.035 0.035 0.035


Konpozisyon chimik ASTM A283:

ASTM A283 Eleman chimik (max) Analiz Chalè, %
Klas C Klas D
Kabòn 0.24 0.27
Manganèz 0.90 0.90
Fosfò 0.030 0.30
Souf 0.030 0.030
Silisyòm    
Plak 11⁄2 pous [40 mm] ak anba, max 0.40 0.40
Plak plis pase 11⁄2 pous [40 mm] 0.15-0.40 0.15-0.40
Kwiv 0.20 0.20

 