ASTM A283 Klas D ASTM A283/A283Mse youn nan pwodwi prensipal yo nan konpayi nou an. Lòt pase ofri kalite siperyè A283 Klas D ak pri konpetitif, nou ede tou rezoud tout kalite dout nan kliyan yo. Tankou A283 Klas D konpozisyon chimik, A283 Klas D pwopriyete, A283 Klas D fòs sede, A283 Klas D fòs rupture, A283 Klas D ekivalan klas, elatriye Pandan se tan, nou menm tou nou fè processing pou ASTM A283 Klas D ASTM A283/A283M, ki gen ladan. koupe, koube, soude, perçage, elatriye.
Aplikasyon:Ba ak mwayen rupture fòs kabòn asye.
Trete chalè:1769 degre - 1847 degre .

ASTM A283 Klas D ASTM A283/A283M Eleman Chimik
Ki konpozisyon chimik ASTM A283 Klas D ASTM A283/A283M? Pou ASTM A283 Klas D ASTM A283/A283M kontni eleman, tanpri kontakte nou.
| Eleman | Min | Maks | Menm jan an |
|---|---|---|---|
| Taks | 0.2000 | - | - |
| P | - | 0.0350 | - |
| S | - | 0.0400 | - |
| Mn | - | 0.9000 | - |
| sizo | 0.1500 | 0.4000 | - |
| C | - | 0.2700 | - |

ASTM A283 klas D ASTM A283/A283M Pwopriyete mekanik
| Sede Rp0.2(MPa) |
Tensile Rm(MPa) |
Enpak KV/Ku (J) |
Elongasyon A (%) |
Rediksyon nan koup transvèsal sou ka zo kase Z (%) |
Kòm-Chalè-trete Kondisyon | Brinell dite (HBW) |
|---|---|---|---|---|---|---|
| 267 (Pi gran pase oswa egal a) | 333 (Pi gran pase oswa egal a) | 24 | 43 | 34 | Solisyon ak Aje, Recuit, Ausaging, Q + T, elatriye | 121 |
ASTM A283 Klas D ASTM A283/A283M Pwopriyete Fizik
Pwopriyete fizik debaz ASTM A283 klas D ASTM A283/A283M Steel
| Tanperati (degre) |
Modil elastisite (GPa) |
Mwayèn koyefisyan ekspansyon tèmik 10-6/( degre ) ant 20( degre ) ak | Konduktivite tèmik (W/m· degre) |
Kapasite tèmik espesifik (J/kg· degre) |
Espesifik rezistans elektrik (Ω mm²/m) |
Dansite (kg/dm³) |
Koyefisyan Poisson a, ν |
|---|---|---|---|---|---|---|---|
| 44 | - | - | 0.34 | - | |||
| 361 | 434 | - | 14.3 | 324 | - | ||
| 898 | - | 34 | 14.2 | 143 | 143 |