ASTM A148 Klas 90-60 ASTM A148/A148M Entwodiksyon
Konpayi nou an se founisè materyèl bwit fè ak asye klas mondyal.ASTM A148 Klas 90-60 ASTM A148/A148Mse youn nan pwodwi prensipal asye nou yo. Lòt pase pwodiksyon fre, nou gen tou gwo aksyon ASTM A148/A148M pou satisfè demann ijan kliyan yo. ASTM A148 Klas 90-60 ASTM A148/A148M disponib nan yon varyete de gwosè estanda epi li kapab tou Customized selon bezwen kliyan yo. Anplis de sa, nou bay sèvis pwosesis, tankou: koupe, koube, perçage, soude ak lòt sèvis pwosesis.
Aplikasyon:Distribisyon asye wo-fòs pou itilizasyon estriktirèl.
Trete chalè:1121 degre - 1361 degre .

ASTM A148 Klas 90-60 ASTM A148/A148M Eleman Chimik
Ki sa ki ASTM A148 Klas 90-60 ASTM A148/A148M fèt? ASTM A148 Klas 90-60 ASTM A148/A148M kontni eleman, ASTM A148 Klas 90-60 Konpozisyon ASTM A148/A148M, ASTM A148 Klas 90-60 ASTM A148/A148M analiz jete
| Eleman | min | Maks | Menm jan an |
|---|---|---|---|
| S | - | 0.0600 | - |
| P | - | 0.0500 | - |

ASTM A148 Klas 90-60 ASTM A148/A148M Pwopriyete mekanik
| Sede Rp0.2(MPa) |
tansyon Rm(MPa) |
Enpak KV/Ku (J) |
Elongasyon A (%) |
Rediksyon nan koup transvèsal sou ka zo kase Z (%) |
Kòm-Chalè-trete Kondisyon | Brinell dite (HBW) |
|---|---|---|---|---|---|---|
| 531 (Pi gran pase oswa egal a) | 296 (Pi gran pase oswa egal a) | 44 | 11 | 24 | Solisyon ak Aje, Recuit, Ausaging, Q + T, elatriye | 312 |
ASTM A148 Klas 90-60 ASTM A148/A148M Pwopriyete Fizik
Pwopriyete fizik debaz ASTM A148 klas 90-60 ASTM A148/A148M Steel
| Tanperati (degre) |
Modil elastisite (GPa) |
Mwayèn koyefisyan ekspansyon tèmik 10-6/( degre ) ant 20( degre ) ak | Konduktivite tèmik (W/m· degre) |
Kapasite tèmik espesifik (J/kg· degre) |
Espesifik rezistans elektrik (Ω mm²/m) |
Dansite (kg/dm³) |
Koyefisyan Poisson a, ν |
|---|---|---|---|---|---|---|---|
| 24 | - | - | 0.13 | - | |||
| 348 | 919 | - | 31.3 | 234 | - | ||
| 196 | - | 23 | 41.2 | 333 | 213 |