12MnNiVR se yon plak asye pou veso presyon. Konpare ak SPV490Q krak sansiblite koyefisyan Pcm nan estanda Japonè JIS G3115 la, li pi ba ak plis fezab soude plak asye. Direksyon echantiyon tès enpak la chanje soti nan lonjitidinal ak transverse, epi tanperati enpak la chanje soti nan -10 degre a - 15 degre oswa pi ba, epi pouvwa enpak la amelyore. 12MnNiVR yo itilize nan fabrikasyon gwo tank depo lwil oliv.
12MnNiVR presyon veso asye plak konpozisyon chimik:
| C | sizo | Mn | P | S | Ni | Kr | Mo | V | PcmMax |
| Mwens pase oswa egal a 0.15 | 0.15~0.4 | 1.2~1.6 | Mwens pase oswa egal a 0.025 | Mwens pase oswa egal a 0.010 | 0.15~0.4 | Mwens pase oswa egal a 0.3 | Mwens pase oswa egal a 0.3 | 0.02~0.06 | Mwens pase oswa egal a 0.26 |