Plak asye 12Cr2Mo1VR fè pati plak asye presyon ba-tanperati, lajman ki itilize nan petwòl sèk, pwodui chimik, estasyon elektrik ak lòt endistri yo. Chodyè ak lòt endistri yo, ak pwodiksyon sèk nan réacteurs, echanjeur chalè, séparateur, tank boul, tank lwil oliv, tank gaz likid petwòl, koki presyon reyaktè nikleyè, louch chodyè, silenn gaz likid, estasyon idwoelektrik tiyo dlo gwo presyon, turbine. turbine ak lòt ekipman ak konpozan.
12Cr2Mo1VR plak asye konpozisyon chimik:
| C | Si | Mn | P | S | Ni | Kr | Mo | Cu | Nb | V | Ti | B | Ca |
| 0.11-0.15 | Mwens pase oswa egal a 0.1 | 0.3-0.6 | Mwens pase oswa egal a 0.010 | Mwens pase oswa egal a 0.005 | Mwens pase oswa egal a 0.25 | 2-2.5 | 0.9-1.1 | Mwens pase oswa egal a 0.2 | Mwens pase oswa egal a 0.07 | 0.25-0.35 | Mwens pase oswa egal a 0.03 | Mwens pase oswa egal a 0.002 | Mwens pase oswa egal a 0.015 |
Pwopriyete mekanik plak asye 12Cr2Mo1VR (epesè: 6-200mm):
| ReL(MPa) | Pi gran pase oswa egal a 415 | Lè rannman an pa evidan, sèvi ak Rp0.2 | |
| Rm (MPa) | 590-760 | ||
| A(%) | Pi gran pase oswa egal a 17 | ||
| Tanperati enpak | -20 | ||
| Akv(J) | Pi gran pase oswa egal a 60 | ||
| Koube dyamèt | 3a | ||
| Koube ang | 180 | ||
| Estati livrezon | nòmalize + apeze | ||