ASTMA285 klas C asyese asye veso komen ak ba oswa mitan{0}}fòs rupture ki ba. Avèk bon pwopriyete ASTM A285 klas C, A285 klas Cplak asyeyo lajman itilize yo bati chodyèr ak veso presyon pou petwòl, endistri chimik ak plant elektrik.
ASTM A285 klas C pwopriyete chimik asye
| Klas | Eleman Max (%) | ||||
| C | Si | Mn | P | S | |
| A285 klas C | 0.28 | 0.08-0.45 | 0.98 | 0.035 | 0.035 |
ASTM A285 klas C asye mekanik pwopriyete
| Klas | Epesè | Sede | Tensile | Elongasyon |
| A285 klas C | mm | Min Mpa | Mpa | % min |
| 6-50 | 205 | 380-515 | 27% | |
| 50-200 | 205 | 380-515 | 23% |
Ki kontni maksimòm fosfò nan A285 klas C
A285 klas C se yon plak asye kabòn yo itilize nan aplikasyon pou veso presyon. Li se souvan itilize nan konstriksyon an nan chodyèr ak tank depo akòz soudabilite bon li yo ak fòs rupture ki ba ak entèmedyè.
Kontni maksimòm fosfò ki espesifye pouA285 klas Cvarye selon epesè plak la. Dapre spesifikasyon ASTM A285, kontni an fosfò maksimòm pèmèt pou plak jiska 1 pous epè se 0.025%. Pou plak plis pase 1 pous epè, kontni an fosfò maksimòm pèmèt se 0.030%.
Fosfò se yon enpurte danjere nan asye ki ka lakòz frajil, diminye severite, ak ogmante risk pou yo fann pandan fabrikasyon ak sèvis. Se poutèt sa, li enpòtan kontwole kontni an fosfò nan asye asire pwopriyete mekanik li yo ak pèfòmans.
Li se vo anyen ke pandan ke spesifikasyon ASTM A285 la bay direktiv pou kontni an fosfò maksimòm nan plak A285 klas C, nivo fosfò aktyèl yo ka varye selon pwosesis fabrikasyon an ak konpozisyon espesifik nan asye a. Li enpòtan pou konsilte dokiman manifakti a pou pwodwi espesifik ke yo te itilize pou detèmine konpozisyon chimik egzak li yo ak pwopriyete yo.
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.


| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Class3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||