High strength steel plates A514 grade E and High strength steel plates A514 grade H owned high yield strength above 690Mpa and high tensile strength within 760-895Mpa,for steel plate A514 grade e and A514 grade H thickness up to 3/4 inches (20mm),the specification A514/A514M requires Brinell Hardness number 235 to 293.
Steel plate A514GRE have a higher Manganese percentage and no requirement contains for Nickel alloy element.However A514grH have a lower Manganese contains and require 0.3-0.7 % contains for Nickel when offering.
|
A514GrEA514GrH |
|
|||||||||||
|
C |
P |
S |
V |
B |
||||||||
|
ASTM A514/A514M |
A514GrE |
0.12-0.20 |
0.4-0.7 |
0.035 |
0.035 |
0.2-0.4 |
/ |
1.4-2.0 |
0.4-0.6 |
/ |
0.01-0.1 |
0.001- 0.005 |
|
ASTM A514/A514M |
A514GrH |
0.12-0.21 |
0.95-1.3 |
0.035 |
0.035 |
0.2-0.35 |
0.3-0.7 |
0.4-0.65 |
0.2-0.3 |
0.03-0.08 |
/ |
0.0005- 0.005 |
|
|
||||||||||||
|
Mpa Min. |
||||||||||||
|
ASTM A514/A514M |
A514GrE |
T<=65 |
690 |
760-895 |
||||||||
|
ASTM A514/A514M |
A514GrH |
T<=65 |
690 |
760-895 |
||||||||