Ki sa ki ekivalan asye ST52 a?

Sep 28, 2025 Kite yon mesaj

ST52-3 klas asyese yon asye manganèz ki ba kabòn ki fasil pou soude ak bon rezistans enpak (tankou tanperati anba -zewo). Materyèl sa a souvan apwovizyone nan kondisyon ki pa trete oswa nòmalize.

 

Konpozisyon chimik nan St52

 

  • Tablo sa yo montre konpozisyon chimik St52.

St52 fèy done asye - 2, Konpozisyon chimik (analiz pwodwi) dapre DIN 17100 ak DIN EN 10025: 1993.

 

 

 

Konpozisyon chimik (analiz pwodwi), %, mwens pase oswa egal a

Peyi (Rejyon)

Estanda

Steel Klas (nimewo Steel)

C

Si

Mn

P

S

N

Cu

Epesè (d) (mm)

Metòd dezoksidasyon

Almay

DIN 17100: 1980

St52-3 (1.0570)

0.22

0.60

1.70

0.065

0.065

 

Mwens pase oswa egal a 30

Totalman Touye

 

0.24

30<="" span="" style="box-sizing: border-box;">

Inyon Ewopeyen an

EN 10025: 1993

S355J2G3 (1.0570)

0.22

0.60

1.70

0.045

0.045

 

Mwens pase oswa egal a 30

0.24

30<="" span="" style="box-sizing: border-box;">

EN 10025-2: 2004

S355J2 (1.0577)

0.22

0.60

1.70

0.035

0.035

0.60

Mwens pase oswa egal a 30

0.24

30<="" span="" style="box-sizing: border-box;">

 

  • Sede fòs

Materyèl St 52-3 Done fèy – 3

 

Fòs sede (Pi gran pase oswa egal a N/mm2); Epesè (d) mm

Steel (nimewo Steel)

d Mwens pase oswa egal a 16

16< d ≤40

40< d ≤63

63< d ≤80

80< d ≤100

>100

St52-3

355

345

335

325

315

pa akò

 

  • Fòs rupture

Materyèl St 52-3 Done fèy – 4

 

Fòs rupture (pi gran pase oswa egal a N/mm2); Epesè (d) mm

Steel (nimewo Steel)

d<3

3 Mwens pase oswa egal a d Mwens pase oswa egal a 100

>100

St 52-3

515-680

490-630

pa akò

Remak: 1MPa=1N/mm2

 

St52 ST 52 Steel Ekivalan Materyèl

 

Materyèl St52 asye ekivalan a Ameriken ASTM AISI SAE, Ewopeyen estanda EN, ISO estanda, Japonè estanda JIS, Chinwa GB estanda ak Ameriken IS estanda. (Pou referans)

Almay

US

Inyon Ewopeyen an

Japon

Lachin

peyi Zend

ISO

Estanda

Steel

Estanda

Steel

Estanda

Steel (nimewo Steel)

Estanda

Steel

Estanda

Steel

Estanda

Steel

Estanda

Steel

DIN 17100: 1980

St 52

ASTM A572/A572M

Klas 50

EN 10025-2: 2005

S355

 

 

GB/T 1591

Q345;
Q355

SE 2062

E350

 

 

St 52-3

 

 

S355J2 (1.0577)

JIS G3135

SPFC590

Q355C; Q345C

 

 

ISO 630-2

S355C

St 52-3U

 

 

S355J0 (1.0553)

 

 

 

 

 

 

 

 