Pwodwi Deskripsyon

 

 

ASTM A285 GRADE C Steel Plakfèt pou chodyèr fizyon soude ak veso presyon, paske li gen bon fòs modere ak fòme pwopriyete.

ASTM A285 GRADE C Steel Plate

Plak asye presyon veso apwovizyone pa GNEE pwodui estrikteman swiv estanda ASTM yo pou delivre klas siperyè plak asye kabòn ki fèt espesyalman pou aplikasyon pou veso presyon ak chofaj ki anplis ekipe pou aplikasyon lajè.

 

Pou veso presyon wo, chodyè, gwo estrikti asye

Lajè: 500mm-4500mm; Epesè: 1.2mm ~ 60mm

Tretman: Cho woule

Sifas: Mill, vèni, prepainted oswa karo

Sètifikasyon: Sètifika tès Mill ak chajman

Pake: Metòd anbalaj estanda ekspòtasyon (anbalaj ki enpèmeyab, pake ak teren asye, palèt asye), anbake ak veso 20 'oswa 40' oswa nan konpayi asirans esansyèl.

 

Klas asye ekivalan nan plak A285 Gr.C

 

 

Britanik estanda Nòm Ewopeyen an ASTM/ASME Espay Almay Japon
161 Gr.360/164 Gr.360 P235GH A/SA285 - Klas C Yon 37 RCI Alo SPV 24

 

Konpozisyon chimik nan ASTM A285 gr.C Kabòn Steel Tensile fòs plak

 

 

ASTM A285 Klas C Konpozisyon Chimik (Pousantaj %)
Klas C Si Mn P S Al Kr Cu Ni Mo Nb Ti V
A285Gr.C 0.16 0.35 0.4/1.2 0.03 0.03 0.02 0.3 0.3 0.3 0.08 0.01 0.03 0.02

 

ASTM A285 Klas C Pwopriyete mekanik

 

 

ASTM A285 Klas C Pwopriyete mekanik
Fòs rupture, [MPa] Fòs sede, min, [MPa] Elongasyon nan anba [50mm], min, %
380-515 205 27

 

 

Metòd Pwosesis komen yo ka fèt sou Plak Veso Presyon ASTM A285 Gr.C

 
  • Koupe
  • Fòme Perçage / Machining
  • Manje
  • Tès

ASTM A285 Gr.C presyon veso Steel Plak gwosè ki disponib

 

 

1/8" 3/8" 3/4" 1-1/2" 3"
3/16" 1/2" 1" 2" 4"
1/4" 5/8" 1-1/4" 2-1/2"  

*1/8" plak epè ki disponib nan yon sèl gwosè sèlman 60"x 120".
Plak epè 3/6" la disponib sèlman kòm 48" x 144"
ak 96" x 144".

 

Mande Yon Quote

 

Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis pase kontan ede w.

 

ASTM A285 Gr.C Pressure Vessel Plate

ASTM A285 Gr.C Pressure Vessel Plate

FAQ

Ki materyèl ki ekivalan a A285?

ASTM se yon wo-klas asye presyon ki gen ekivalanKlas Ewopeyen an se P235GH, ak estanda Britanik ki gen klas 161 Gr. 360/164 Gr. 360.

Steel Klas EN 10028-2 BS 1501
ASTM A285GradeA B C P235GH 161 Gr. 360164 Gr. 360

 

Ki spesifikasyon ASTM A285?

Espesifikasyon ASTM A285 se spesifikasyon estanda pou plak veso presyon, asye kabòn, ba - ak entèmedyè-fòs rupture ki fèt pou fizyon-veso presyon soude. Twa klas ki gen diferan nivo fòs yo disponib nan epesè jiska 2 ", enklizif.

 

Ki diferans ki genyen ant asye A285 ak A36?

A285 Klas C gen fòs rupture ki ba ak mwayen ant 380 a 515 MPa, tandiske fòs rupture nan materyèl A36 varye ant 400 a 500 MPa. Sa a se akòz varyasyon nan konpozisyon chimik yo.

 

Ki diferans ki genyen ant ASTM A285 ak A516?

ASTM A516 ofri pi gwo fòs epi li apwopriye pou aplikasyon pou presyon modere-a-wo, pandan y ap ASTM A285 se pri -efikas ak ideyal pou anviwònman presyon ba-. ASTM A516 ak ASTM A537 yo fèt espesyalman pou wo -tanperati ak presyon veso aplikasyon.

 

Klas Plak Veso Presyon Apwovizyone Pa GNEE
ASTM ASTM A202/A202M ASTM A202 Klas A ASTM A202 Klas B    
ASTM A203/A203M ASTM A203 Klas A ASTM A203 Klas B ASTM A203 Klas D ASTM A203 Klas E
ASTM A203 Klas F      
ASTM A204/A204M ASTM A204 Klas A ASTM A204 Klas B ASTM A204 Klas C  
ASTM A285/A285M ASTM A285 Klas A ASTM A285 Klas B ASTM A285 Klas C  
ASTM A299/A299M ASTM A299 Klas A ASTM A299 Klas B    
ASTM A302/A302M ASTM A302 Klas A ASTM A302 Klas B ASTM A302 Klas C ASTM A302 Klas D
ASTM A387/A387M ASTM A387 Klas 5 Klas1 ASTM A387 Klas 5 Klas2 ASTM A387 Klas 11 Klas1 ASTM A387 Klas 11 Klas2
ASTM A387 Klas 12 Klas1 ASTM A387 Klas 12 Klas2 ASTM A387 Klas 22 Klas1 ASTM A387 Klas 22 Klas2
ASTM A515/A515M ASTM A515 Klas 60 ASTM A515 Klas 65 ASTM A515 Klas 70  
ASTM A516/A516M ASTM A516 Klas 55 ASTM A516 Klas 60 ASTM A516 Klas 65 ASTM A516 Klas 70
ASTM A517/A517M ASTM A517 Klas A ASTM A517 Klas B ASTM A517 Klas E ASTM A517 Klas F
ASTM A517 Klas P ASTM A517 klas J    
ASTM A533/A533M ASTM A533 Klas A Klas 1 ASTM A533 Klas B Klas1 ASTM A533 Klas C Class1 ASTM A533 Klas D Class1
ASTM A533 Klas A Klas2 ASTM A533 Klas B Klas2 ASTM A533 Klas C Class2 ASTM A533 Klas D Klas2
ASTM A533 Klas A Klas3 ASTM A533 Klas B Klas3 ASTM A533 Klas C Class3 ASTM A533 Klas D Class3
ASTM A537/A537M ASTM A537 Klas 1 ASTM A537 Klas 2 ASTM A537 Klas 3  
ASTM A612/A612M ASTM A612      
ASTM A662/A662M ASTM A662 Klas A ASTM A662 Klas B ASTM A662 Klas C  
EN EN10028-2 EN10028-2 P235GH EN10028-2 P265GH EN10028-2 P295GH EN10028-2 P355GH
EN10028-2 16MO3      
EN10028-3 EN10028-3 P275N EN10028-3 P275NH EN10028-3 P275NL1 EN10028-3 P275NL2
EN10028-3 P355N EN10028-3 P355NH EN10028-3 P355NL1 EN10028-3 P355NL2
EN10028-3 P460N EN10028-3 P460NH EN10028-3 P460NL1 EN10028-3 P460NL2
EN10028-5 EN10028-5 P355M EN10028-5 P355ML1 EN10028-5 P355ML2 EN10028-5 P420M
EN10028-5 P420ML1 EN10028-5 P420ML2 EN10028-5 P460M EN10028-5 P460ML1
EN10028-5 P460ML2      
EN10028-6 EN10028-6 P355Q EN10028-6 P460Q EN10028-6 P500Q EN10028-6 P690Q
EN10028-6 P355QH EN10028-6 P460QH EN10028-6 P500QH EN10028-6 P690QH
EN10028-6 P355QL1 EN10028-6 P460QL1 EN10028-6 P500QL1 EN10028-6 P690QL1
EN10028-6 P355QL2 EN10028-6 P460QL2 EN10028-6 P500QL2 EN10028-6 P690QL2
JIS JIS G3115 JIS G3115 SPV235 JIS G3115 SPV315 JIS G3115 SPV355 JIS G3115 SPV410
JIS G3115 SPV450 JIS G3115 SPV490    
JIS G3103 JIS G3103 SB410 JIS G3103 SB450 JIS G3103 SB480 JIS G3103 SB450M
JIS G3103 SB480M      
GB GB713 GB713 Q245R GB713 Q345R GB713 Q370R GB713 12Cr1MoVR
GB713 12Cr2Mo1R GB713 13MnNiMoR GB713 14Cr1MoR GB713 15CrMoR
GB713 18MnMoNbR      
GB3531 GB3531 09MnNiDR GB3531 15MnNiDR GB3531 16MnDR  
DIN DIN 17155 DIN 17155 HI DIN 17155 HII DIN 17155 10CrMo910 DIN 17155 13CrMo44
DIN 17155 15Mo3 DIN 17155 17Mn4 DIN 17155 19Mn6