DIN 17155 15Mo3se yon kalite plak asye alyaj ki espesifye pa kounye a -demode estanda Alman DIN 17155 la. Li se yon klas kabòn-molybdène ki itilize pou fabrikasyon chodyè ak veso presyon ki opere nan tanperati ki wo. Li ekivalan a estanda modèn EN 10028-2 16Mo3, ak konpozisyon chimik li gen ladan kabòn, Manganèz, ak molybdène.
DIN 17155 15Mo3 presyon veso ak chodyè asye plak konpozisyon chimik ak pwopriyete mekanik
|
15Mo3 konpozisyon chimik |
|||||||
|
Klas |
Eleman Max (%) |
||||||
|
15Mo3 |
C |
Si |
Mn |
P |
S |
Al |
Kr |
|
0.12-0.20 |
0.10-0.35 |
0.40-0.90 |
0.035 |
0.030 |
|
0.25 |
|
|
Cu |
Ni |
Mo |
Nb |
Ti |
V |
|
|
|
0.3 |
0.3 |
0.25-0.35 |
|
|
|
|
|
|
Klas |
15Mo3 Pwopriyete mekanik |
|
|
Epesè |
Sede |
|
|
15Mo3 |
mm |
Min Mpa |
|
6-16 |
275 |
|
|
16-40 |
270 |
|
|
40-60 |
260 |
|
|
60-100 |
240 |
|
|
100-150 |
220 |
|
DIN 17155 15Mo3 Presyon Veso ak Chodyè Steel Plak Aplikasyon

Veso reyaksyon chimik
DIN 17155 15Mo3 chodyè ak presyon veso asye plak yo itilize nan reyaksyon sentèz (tankou gwo fò tou won sentèz amonyak nan plant angrè ak réacteurs polymérisation nan plant chimik). Li bezwen kenbe tèt ak tanperati ki wo ak presyon (egzanp, gwo kay won an sentèz amonyak opere nan yon presyon nan 30MPa ak yon tanperati nan 450 degre) ak korozyon mwayen (tankou idwojèn ak gaz asid) asire ke pa gen okenn flit oswa echèk estriktirèl rive pandan pwosesis reyaksyon an.
Tank Depo Petrochimik ak gwo fò tou won
DIN 17155 15Mo3 Low Tanperati Presyon Vessel Steel Plate yo itilize nan tank depo pou lwil brit, gaz natirèl likid (LNG), ak gaz petwòl likid (LPG), osi byen ke gwo fò tou won redresman ak gwo fò tou won absòpsyon nan raffinage petwòl: tanperati nòmal ak tank depo presyon (tankou tank lwil brit); tank depo tanperati ki ba -(tankou tank depo LNG, ak tanperati ki ba ke -162 degre) mande pou plak asye ak ekselan rezistans tanperati ba-pou evite frajil ka zo kase asye nan tanperati ki ba; gwo fò tou won idrojenasyon wo-presyon (pwosesis hydrofining pétrochimique).
Veso echanj chalè
DIN 17155 15Mo3 High-Boiler Steel Plate yo itilize nan ekipman pou echanj chalè mwayen (tankou echanjeur chalè-ak-tib ak echanjeur chalè plak). Koki yo ak fèy tib yo bezwen kenbe tèt ak altène chok cho ak frèt, asire rezistans fatig, epi evite fann soude ki te koze pa chanjman tanperati souvan.
Endistri metaliji
"Explosif founo cho eksplozyon recho" nan plant asye (ki estoke gwo -tanperati lè cho, ak yon presyon 0.5-1.5MPa ak yon tanperati 1200 degre ) sèvi ak segondè -tanperati DIN 17155 15Mo3 cho- plak woule; "Otoklav la" nan fusion metal ki pa FERROUS (tankou otoklav la lesivaj nan fusion kwiv idrometallurgik) bezwen yo dwe rezistan a korozyon asid, ak DIN 17155 15Mo3 presyon veso asye plak yo souvan itilize.
DIN 17155 15Mo3 Presyon Veso ak Chodyè Steel Plak Lòt Non
DIN 17155 15Mo3 Chodyè plak asye, DIN 17155 15Mo3 Presyon Veso Steel plak, DIN 17155 15Mo3 Tank Depo Steel plak. DIN 17155 15Mo3 Chalè Echanjeur Steel Plak .
Kondisyon adisyonèl
UT (Egzamen Ultrasonic), AR (Kòm woule cho sèlman), TMCP (Tèmik Pwosesis kontwòl mekanik), N (Normalize), Q + T (Tenn ak Tanperaman), Tès Direksyon Z (Z15, Z25, Z35), Tès Enpak Charpy V - Notch, Tès Twazyèm Pati (tankou Tès SGS), kouvwi ak pating.
Klike pou jwenn yon echantiyon gratis
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.
Ki sa ki ekivalan din 15Mo3 a?
EN 16Mo3
DIN 15Mo3 se EN 16Mo3 klas ekivalan. Li fasil sonje ke konpozisyon chimik la ak pwopriyete mekanik 16Mo3 asye ak EN 16Mo3 klas ekivalan DIN 15Mo3 yo prèske menm bagay la. Yo parfe ekivalan youn ak lòt.
Ki sa ki materyèl 15Mo3?
An konklizyon, tib asye 15Mo3 se yon inik -alyaj asye ki gen molybdène ak chromium. Pwopriyete fizik li yo fè li apwopriye pou aplikasyon pou gwo -tanperati, ak konpozisyon chimik li yo ba li ekselan rezistans korozyon.
Ki sa ki se 15Mo3 ekivalan ASME materyèl?
Materyèl 15mo3 yo itilize nan aplikasyon ki gen tanperati ki wo tankou echanjeur chalè ak veso presyon, epi yo ekivalan a UNI5869 15Mo3 ak EN10028 16Mo3, ASTM A204Gr. B ak 15D3 (NFA 36205).
Ki sa ki diferan ant 15Mo3 ak 16Mo3 asye?
15Mo3 ak 16Mo3 asye yo se chodyè asye, yo ka itilize pou chodyè oswa presyon vessel.but 15Mo3 asye anba DIN 17155 estanda, 16Mo3 asye anba estanda EN10028. ak 15Mo3 asye ki ekivalan a GB5310, ASME SA210, ASME SA213, DIN17175.
15Mo3 asye konpozisyon chimik:
| Klas | C. max | Mn. | S. | N | Cu | Si. | P. | Kr. | Ni. | Mo. |
| 15Mo3 | 0.12- 0.2 | 0.40- 0.90 | 0.01 | 0.012 | 0.30 | 0.35 | 0.025 | 0.30 | 0.30 | 0.25- 0.35 |
16Mo3 asye Chimik Konpozisyon
| Klas | C | Si | Mn | P | S | Kr | Mo | Ni | Nb | Ti | V | Al | N | Cu |
| 16Mo3 | 0.12/0.20 | 0.35 | 0.40/0.90 | 0.025 | 0.010 | 0.030 | 0.25/0.35 | 0.30 | – | – | – | – | 0.012 | 0.30 |
| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Class3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||