P355Q ak P460Q se klas ki trempe ak tanperaman soude amann grenn asye yo itilize pou veso presyon ak ekipman tanperati ki wo, dapre estanda EN 10028-6. Diferans prensipal la se fòs yo: P460Q se yon klas fòs ki pi wo pase P355Q.
Teknoloji Siplemantè: Tès HIC|NACE MR0175|Z15|Z25|Z35 |
Epesè: 6MM a 300MM,
Lajè: 1500mm a 4050mm,
Longè: 3000mm a 15000mm

|
P355Q konpozisyon chimik |
|||||||
|
Klas |
Eleman Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
N |
B |
|
|
P355Q |
0.16 |
0.4 |
1.5 |
0.025 |
0.015 |
0.015 |
0.005 |
|
Mo |
Cu |
Nb |
Ni |
Ti |
V |
Zr |
|
|
0.25 |
0.3 |
0.05 |
0.5 |
0.03 |
0.06 |
0.05 |
|
Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
P460Q konpozisyon chimik |
|||||||
|
Klas |
Eleman Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
N |
B |
|
|
P460Q |
0.18 |
0.50 |
1.70 |
0.025 |
0.015 |
0.015 |
0.005 |
|
Mo |
Cu |
Nb |
Ni |
Ti |
V |
Zr |
|
|
0.50 |
0.3 |
0.05 |
0.5 |
0.03 |
0.06 |
0.05 |
|
Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
Klas |
P355Q Pwopriyete mekanik |
|||
|
Epesè |
Sede |
Tensile |
Elongasyon |
|
|
P355Q |
mm |
Min Mpa |
Mpa |
% min |
|
6-50 |
355 |
490-630 |
22% |
|
|
50-100 |
335 |
490-630 |
22% |
|
|
100-150 |
315 |
450-590 |
22% |
|
|
Klas |
P460Q Pwopriyete mekanik |
|||
|
Epesè |
Sede |
Tensile |
Elongasyon |
|
|
P460Q |
mm |
Min Mpa |
Mpa |
% min |
|
6-50 |
460 |
550-720 |
19% |
|
|
50-100 |
440 |
550-720 |
19% |
|
|
100-150 |
400 |
500-670 |
19% |
|