Weldable estriktirèl asye SM490A, SM490A plak asye, SM490A fèy asye se anba asye estanda JIS G3106.Pou epesè nan plak asye egal oswa anba 16mm, fòs la sede minimòm pou asye plak sm490a yo dwe pi wo pase 325mpa, pou epesè ki genyen ant 16mm ak 40mm, sede minimòm la dwe 315 mPa nan mPa a, epi yo ka animè minim minimè a, epi yo ka gen 31 mm minim minimè a, epi yo ka gen 31 mm, epi yo ka gen 31 mm, epi yo te gen yon bagay ki pi wo pase. SM490A dwe 295 MPA.As fòs la rupture nan asye plak SM490A yo dwe nan 490-610 MPa pou epesè a egal ak anba a 100mm, ak 400-610 MPa pou epesè ki pi wo a 100mm.

►Pwopriyete mechnical pou plak asye SM490A:
| Epesè (mm) | |||||||
| SM490A | Mwens pase oswa egal a 16 | >16 mwens pase oswa egal a 40 | >40 mwens pase oswa egal a 75 | >75 mwens pase oswa egal a 100 | >100 mwens pase oswa egal a 160 | > 160 | |
| Sede fòs (pi gran pase oswa egal a MPa) | 325 | 315 | 295 | 295 | 285 | 275 | |
| Mwens pase oswa egal a 100 | > 100 | ||||||
| Fòs rupture (MPa) | 490-610 | 400-610 | |||||
►Konpozisyon chimik pou plak asye SM490A (analiz louch max%)
| Main eleman chimik konpozisyon nan plak asye SM490A | |||||
| Epesè (mm) | C | Si | Mn | P | S |
| T mwens pase oswa egal a 50 | 0.20 | 0.55 | 1.60 | 0.035 | 0.035 |
| 50<> | 0.22 | ||||

SM490A ekivalan
|
Lerop |
Fè |
Almay |
Fran |
Itali |
Sil |
Peyi pwovizwa |
USA |
U.K |
|
S 355 Jr |
AE 355 B |
|
E 36-2 |
Fe 510 B |
Ss21,32,01 |
IS 961 |
A633 Gr A, C, D |
50 B |