S890Q segondè fòs asye plak
S890Q-wo fòs alyaj plak se yon materyèl asye-wo fen ki gen gwo fòs, segondè severite, bon pèfòmans soude ak rezistans korozyon.
Plak asye alyaj S890Q toujou kenbe severite bon nan anviwònman tanperati ki ba, gen severite enpak ekselan, epi li apwopriye pou divès kalite pwosesis soude. Nan anviwònman korozivite tankou anviwònman maren ak atmosfè endistriyèl, plak asye S890Q wo-fòs ka efektivman reziste korozyon ak pwolonje lavi sèvis.
Plak asye alyaj S890Q wo-fòs lajman ki itilize nan sipò idwolik min chabon, machin lou, machin jeni ak lòt estrikti asye ki mande pou bon pèfòmans soude.
Konpozisyon chimik % asye S890Q (1.8940): EN 10025-6-2004
| C | Si | Mn | Ni | P | S | Kr | Mo | V | N | Nb | Ti | Cu | Zr | B | CEV |
| max 0.2 | max 0.8 | maksimòm 1.7 | max 2 | max 0.025 | max 0.015 | maksimòm 1.5 | max 0.7 | max 0.12 | max 0.015 | max 0.06 | max 0.05 | max 0.5 | max 0.15 | max 0.005 | max 0.82 |
Pwopriyete mekanik asye S890Q (1.8940)
| Epesè nominal (mm): | 3 - 50 | 50 - 100 |
| Rm- Fòs rupture (MPa) | 940-1100 | 880-1100 |
| Epesè nominal (mm): | 3 - 50 | 50 - 100 |
| ReH- Minimòm fòs sede (MPa) | 890 | 830 |
| KV- Enèji enpak (J) lonjitid., | 0 degre 40 |
-20 degre 30 |
| A- Min. elongasyon Lo=5,65 √ So (%) | 11 |
| Non pwodwi | Segondè fòs ki ba alyaj asye plak (HSLA) |
| Longè | 1m-12m oswa jan sa nesesè |
| Lajè | 1m-3m oswa jan sa nesesè |
| Epesè | 8mm-150mm oswa jan sa nesesè |
| Estanda | ASME, ASTM, DIN, JIS, GB, EN, elatriye. |
| Teknik | Woule cho |
| Tretman andigman | Netwaye, eksplozif ak penti selon kondisyon kliyan |
| Tolerans epesè | ±0.1mm |
| Materyèl |
ASTM: A573 Klas 70, A709 Klas 50, A514 Klas B, elatriye. ASME:SA573 Klas 70,SA709 Klas 50,SA514 Klas B, elatriye. EN:S355JR,S355J0,S355K2,S355N,S355J2,S420N,S460N, S460Q, S460QL, S500Q, S500QL, S550Q, S500QL, S690Q, S690QL, S690QL1, S890Q, S890QL, S890QL1, S960Q, S960QL, elatriye. DIN:ST52-3, elatriye. JIS:SS490,SS540,SM490, elatriye. GB:Q355B,Q355D,Q390B,Q390D,Q420B,Q420D, Q460D,Q460E,Q500D,Q500E,Q550D,Q550E, Q620D, Q620E, Q690D, Q690E, Q890D, Q890E, Q960D, Q960E, elatriye. |
| MOQ | 1tons.We tou ka aksepte echantiyon lòd. |
| Tan chajman | Nan 15-30 jou travay apre yo fin resevwa depo oswa L/C |
| Ekspòtasyon anbalaj | Papye ki enpèmeyab, ak teren asye chaje. Creole Export Seaworthy Package.Suit pou tout kalite transpò, oswa jan sa nesesè |